CATIONIC ELECTRO-DEPOSITION COATING COMPOSITION
To provide a cationic electro-deposition coating composition which exhibits higher corrosion resistance, and good performance, especially, even in a cycle corrosion test.SOLUTION: A cationic electro-deposition coating composition contains an aminated epoxy resin, a blocked polyisocyanate curing agen...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide a cationic electro-deposition coating composition which exhibits higher corrosion resistance, and good performance, especially, even in a cycle corrosion test.SOLUTION: A cationic electro-deposition coating composition contains an aminated epoxy resin, a blocked polyisocyanate curing agent, and a polyamine polymer having an N-substituted diallylamine segment. The polyamine polymer has an N-substituted diallylamine segment represented by the following formula (1), or its acid addition salt. In the formula (1), p and q represent 0 or 1, when p is 1, q is 0, and when p is 0, q is 1; and R1 is the same or different, and represents an alkyl group which may have a hydroxyl group and has 1 to 10 carbon atoms or an aralkyl group having 7 to 10 carbon atoms.SELECTED DRAWING: None
【課題】より高い防食性、特にサイクル腐食試験でも良好な性能を示すカチオン電着塗料組成物を提供する。【解決手段】アミン化エポキシ樹脂、ブロック化ポリイソシアネート硬化剤およびN置換ジアリルアミンセグメントを有するポリアミン重合体を含有するカチオン電着塗料組成物を提供する。ポリアミン重合体は、下記式:TIFF2022129791000017.tif3777(式中、pおよびqはいずれも0または1を示し、pが1の時にはqは0で、pが0の時にはqは1である。R1は、同一または異なって、水酸基を有してもよい炭素数1~10のアルキル基または炭素数7~10のアラルキル基を示す。)で表されるN置換ジアリルアミンセグメントまたはその酸付加塩を有する。【選択図】なし |
---|