ELECTROSEAMED STEEL PIPE, AND PRODUCTION METHOD OF ELECTROSEAMED STEEL PIPE
To provide an electroseamed steel pipe having high intensity and excellent low-temperature toughness.SOLUTION: An electroseamed steel pipe is composed of predetermined components and has a component composition of a ratio Mn/Si of Mn content to Si content higher than 36, a fine structure composed of...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide an electroseamed steel pipe having high intensity and excellent low-temperature toughness.SOLUTION: An electroseamed steel pipe is composed of predetermined components and has a component composition of a ratio Mn/Si of Mn content to Si content higher than 36, a fine structure composed of a bainite phase and a ferrite phase of an area ratio of 10% or less, and mechanical characteristics of a tensile strength of 780 MPa or more and a Charpy absorption energy of 31 J or more at -20°C.SELECTED DRAWING: None
【課題】高強度かつ低温靭性に優れた電縫鋼管を提供する。【解決手段】所定の成分からなり、かつSi含有量に対するMn含有量の比Mn/Siが36超である成分組成を有し、ベイナイト相と、面積率10%以下のフェライト相からなる微細組織を有し、引張強度が780MPa以上、-20℃におけるシャルピー吸収エネルギーが31J以上である機械的特性を有する、電縫鋼管。【選択図】なし |
---|