AUSTENITIC STAINLESS STEEL SHEET AND STEEL PIPE AND METHOD FOR PRODUCING THE SAME
To provide an austenitic stainless steel sheet and steel pipe having high resistance to hydrogen embrittlement and hot crack, and a method for producing the same.SOLUTION: An austenitic stainless steel sheet has a chemical composition consisting of, in mass%, C: 0.10% or less, Si: 1.0% or less, Mn:...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide an austenitic stainless steel sheet and steel pipe having high resistance to hydrogen embrittlement and hot crack, and a method for producing the same.SOLUTION: An austenitic stainless steel sheet has a chemical composition consisting of, in mass%, C: 0.10% or less, Si: 1.0% or less, Mn: 8.0-10.0%, P: 0.030% or less, S: 0.0030% or less, Cr: 15.0-18.0%, Ni: 7.0-9.0%, N: 0.15-0.25%, Al: 0.005-0.20%, Ca: 0.0005-0.01%, B: 0.0002-0.01%, Mg: 0.0001-0.0050%, Cu: less than 1.0%, Mo: 0.5% or less, O: 0.0050% or less, an optional element, with the balance being Fe and impurities. An f value, calculated by [Ni+0.72Cr+0.88Mo+1.11Mn-0.27Si+12.93C+7.55N], is more than 29.5 to less than 32.5.SELECTED DRAWING: None
【課題】耐水素脆化性と耐高温割れ性とに優れたオーステナイト系ステンレス鋼板および鋼管ならびにこれらの製造方法を提供する。【解決手段】化学組成が、質量%で、C:0.10%以下、Si:1.0%以下、Mn:8.0~10.0%、P:0.030%以下、S:0.0030%以下、Cr:15.0~18.0%、Ni:7.0~9.0%、N:0.15~0.25%、Al:0.005~0.20%、Ca:0.0005~0.01%、B:0.0002~0.01%、Mg:0.0001~0.0050%、Cu:1.0%未満、Mo:0.5%以下、O:0.0050%以下、任意元素、残部:Feおよび不純物であり、[Ni+0.72Cr+0.88Mo+1.11Mn-0.27Si+12.93C+7.55N]で算出されるf値が、29.5超32.5未満である、オーステナイト系ステンレス鋼板。【選択図】なし |
---|