POLYAMIDE-IMIDE SOLUTION FOR BELT MOLDING AND METHOD OF MANUFACTURING POLYAMIDE-IMIDE BELT

To provide a PAI solution capable of manufacturing a polyamide-imide (PAI) belt having excellent thickness uniformity and excellent mechanical characteristics, and to provide a method of manufacturing the PAI belt using the same.SOLUTION: (1) Disclosed is a PAI solution for belt molding, which is a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YOSHINO FUMIKO, SHIBATA KENTA, MORIKITA TATSUYA, ECHIGO YOSHIAKI, SHIGETA AKIRA
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To provide a PAI solution capable of manufacturing a polyamide-imide (PAI) belt having excellent thickness uniformity and excellent mechanical characteristics, and to provide a method of manufacturing the PAI belt using the same.SOLUTION: (1) Disclosed is a PAI solution for belt molding, which is a solution containing trimellitic acid as an acid component and PAI using an o-tolidine diisocyanate as an isocyanate component, whose viscosity is 60 Pa s or more and 200 Pa s or less, and whose concentration is more than 15 mass% and less than 25 mass%. (2) Disclosed is a method of manufacturing a PAI belt which is characterized in that the PAI solution is applied to a cylindrical mold and the cylindrical mold is demolded after being dried.SELECTED DRAWING: None 【課題】良好な厚み均一性を有し、かつ力学的特性が良好なポリアミドイミド(PAI)ベルトが作成できるPAI溶液およびこれを用いたPAIベルトの製造方法の提供。【解決手段】<1> 酸成分としてトリメリット酸、イソシアネート成分としてo-トリジンジイソシアネートを用いたPAIを含む溶液であって、粘度が60Pa・s以上、200 Pa・s以下であり、濃度が15質量%超、25質量%未満であるベルト成形用PAI溶液。<2> 前記PAI溶液を、円筒状金型に塗布、乾燥後、脱型することを特徴とするPAIベルトの製造方法。【選択図】なし