Li2O-Al2O3-SiO2-BASED CRYSTALLIZED GLASS AND Li2O-Al2O3-SiO2-BASED CRYSTALLINE GLASS
To provide a Li2O-Al2O3-SiO2-based crystallized glass that has an excellent impact strength and thermal shock strength even if the amount of lithium-containing raw material used is reduced.SOLUTION: The Li2O-Al2O3-SiO2-based crystallized glass and a Li2O-Al2O3-SiO2-based crystalline glass contain, i...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide a Li2O-Al2O3-SiO2-based crystallized glass that has an excellent impact strength and thermal shock strength even if the amount of lithium-containing raw material used is reduced.SOLUTION: The Li2O-Al2O3-SiO2-based crystallized glass and a Li2O-Al2O3-SiO2-based crystalline glass contain, in mass percentage, 60.0 to 70.0% SiO2, 15.0 to 25.0% Al2O3, 1.0 to 6.0% Li2O, 1.0 to 4.0% TiO2, 0.5 to 3.0% ZrO2, 0.1 to 3.0% MnO2, 0.1 to 2.0% Na2O, 0.1 to 2.0% K2O, 0.1 to 2.0% P2O5, 0.1 to 1.5% MgO, 0.1 to 3.0% ZnO, 0.1 to 2.5% BaO and 0.1 to 1.5% As2O3.SELECTED DRAWING: None
【課題】リチウムを含有する原料の使用量を減らしても、衝撃強度と熱衝撃強度とに優れるLi2O−Al2O3−SiO2系結晶化ガラスを提供する。【解決手段】Li2O−Al2O3−SiO2系結晶化ガラス及びLi2O−Al2O3−SiO2系結晶性ガラスは、質量百分率で、SiO260.0〜70.0%、Al2O315.0〜25.0%、Li2O 1.0〜6.0%、TiO21.0〜4.0%、ZrO20.5〜3.0%、MnO20.1〜3.0%、Na2O 0.1〜2.0%、K2O 0.1〜2.0%、P2O50.1〜2.0%、MgO 0.1〜1.5%、ZnO 0.1〜3.0%、BaO 0.1〜2.5%及びAs2O30.1〜1.5%を含む。【選択図】なし |
---|