FERRITE CALCINED BODY, FERRITE SINTERED MAGNET AND MANUFACTURING METHOD THEREOF

To provide a ferrite calcined body and a ferrite sintered magnet which have high Br and less decrease in HcJ, and in which the usage amount of Co and La is more reduced than conventional Ca-La-Co ferrite sintered magnets, and a manufacturing method thereof.SOLUTION: In a ferrite calcined body, the a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: TANIOKU YASUAKI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To provide a ferrite calcined body and a ferrite sintered magnet which have high Br and less decrease in HcJ, and in which the usage amount of Co and La is more reduced than conventional Ca-La-Co ferrite sintered magnets, and a manufacturing method thereof.SOLUTION: In a ferrite calcined body, the atomic ratio of metallic elements of Ca, R, A, Fe, Co and Zn (where, R represents an element which is at least one of rare earth elements and which essentially contains La, and A represents Sr and/or Ba) is represented by general formula: Ca1-x-x'RxAx'Fe2n-y-zCoyZnz where the x, x', y and z, and the n (provided that 2n is a molar ratio and represented as 2n=(Fe+Co+Zn)/(Ca+R+A))satisfy 0.40≤x