TITANIUM ALLOY SHEET, AND EXHAUST SYSTEM COMPONENTS FOR AUTOMOBILE

To provide a titanium alloy sheet in which coarsening of crystal grains is suppressed under a high-temperature environment, and high-temperature strength is excellent.SOLUTION: A titanium alloy sheet contains Cu, Sn, Si, Nb and Al, contains one or both of Cr and Mo, Fe and O are limited to 0.06% or...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAKEBE HIDENORI, NISHIWAKI SOSUKE, KAWAKAMI AKIRA
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TAKEBE HIDENORI
NISHIWAKI SOSUKE
KAWAKAMI AKIRA
description To provide a titanium alloy sheet in which coarsening of crystal grains is suppressed under a high-temperature environment, and high-temperature strength is excellent.SOLUTION: A titanium alloy sheet contains Cu, Sn, Si, Nb and Al, contains one or both of Cr and Mo, Fe and O are limited to 0.06% or less and 0.07% or less respectively, contains one or two or more kinds of Ni, V, Mn, Zr, Co, Ta, W, C and N by 0.3% or less in total, balance is Ti and impurities, in which a metallic structure consists of an α phase and a second phase, the average crystal grain diameter of the α phase is 10 to 50 μm, and the number of measurement areas having the number density 0.01 piece/μm2 or more is 80% or more of all measurement areas.SELECTED DRAWING: None 【課題】高温環境下で結晶粒の粗大化が抑制され、高温強度に優れたチタン合金板を提供する。【解決手段】Cu、Sn、Si、Nb、Alを含有し、Cr、Moの一方または両方を含有し、Feを0.06%以下、Oを0.07%以下に制限し、Ni、V、Mn、Zr、Co、Ta、W、C、Nの1種または2種以上を合計で0.3%以下含有し、残部がTi及び不純物であり、金属組織がα相と第二相からなり、α相の平均結晶粒径が10〜50μmであり、個数密度が0.01個/μm2以上の測定領域の数が全測定領域の80%以上であるチタン合金板を採用する。【選択図】なし
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2021028407A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2021028407A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2021028407A3</originalsourceid><addsrcrecordid>eNrjZHAK8Qxx9PMM9VVw9PHxj1QI9nB1DdFRcPRzUXCN8HAMDQ5RCI4MDnH1VXD29w3w93P1CwlWcPMPUnAMDfH39Xfy9HHlYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBkaGBkYWJgbmjsZEKQIAcIcr2g</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>TITANIUM ALLOY SHEET, AND EXHAUST SYSTEM COMPONENTS FOR AUTOMOBILE</title><source>esp@cenet</source><creator>TAKEBE HIDENORI ; NISHIWAKI SOSUKE ; KAWAKAMI AKIRA</creator><creatorcontrib>TAKEBE HIDENORI ; NISHIWAKI SOSUKE ; KAWAKAMI AKIRA</creatorcontrib><description>To provide a titanium alloy sheet in which coarsening of crystal grains is suppressed under a high-temperature environment, and high-temperature strength is excellent.SOLUTION: A titanium alloy sheet contains Cu, Sn, Si, Nb and Al, contains one or both of Cr and Mo, Fe and O are limited to 0.06% or less and 0.07% or less respectively, contains one or two or more kinds of Ni, V, Mn, Zr, Co, Ta, W, C and N by 0.3% or less in total, balance is Ti and impurities, in which a metallic structure consists of an α phase and a second phase, the average crystal grain diameter of the α phase is 10 to 50 μm, and the number of measurement areas having the number density 0.01 piece/μm2 or more is 80% or more of all measurement areas.SELECTED DRAWING: None 【課題】高温環境下で結晶粒の粗大化が抑制され、高温強度に優れたチタン合金板を提供する。【解決手段】Cu、Sn、Si、Nb、Alを含有し、Cr、Moの一方または両方を含有し、Feを0.06%以下、Oを0.07%以下に制限し、Ni、V、Mn、Zr、Co、Ta、W、C、Nの1種または2種以上を合計で0.3%以下含有し、残部がTi及び不純物であり、金属組織がα相と第二相からなり、α相の平均結晶粒径が10〜50μmであり、個数密度が0.01個/μm2以上の測定領域の数が全測定領域の80%以上であるチタン合金板を採用する。【選択図】なし</description><language>eng ; jpn</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2021</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210225&amp;DB=EPODOC&amp;CC=JP&amp;NR=2021028407A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76419</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20210225&amp;DB=EPODOC&amp;CC=JP&amp;NR=2021028407A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TAKEBE HIDENORI</creatorcontrib><creatorcontrib>NISHIWAKI SOSUKE</creatorcontrib><creatorcontrib>KAWAKAMI AKIRA</creatorcontrib><title>TITANIUM ALLOY SHEET, AND EXHAUST SYSTEM COMPONENTS FOR AUTOMOBILE</title><description>To provide a titanium alloy sheet in which coarsening of crystal grains is suppressed under a high-temperature environment, and high-temperature strength is excellent.SOLUTION: A titanium alloy sheet contains Cu, Sn, Si, Nb and Al, contains one or both of Cr and Mo, Fe and O are limited to 0.06% or less and 0.07% or less respectively, contains one or two or more kinds of Ni, V, Mn, Zr, Co, Ta, W, C and N by 0.3% or less in total, balance is Ti and impurities, in which a metallic structure consists of an α phase and a second phase, the average crystal grain diameter of the α phase is 10 to 50 μm, and the number of measurement areas having the number density 0.01 piece/μm2 or more is 80% or more of all measurement areas.SELECTED DRAWING: None 【課題】高温環境下で結晶粒の粗大化が抑制され、高温強度に優れたチタン合金板を提供する。【解決手段】Cu、Sn、Si、Nb、Alを含有し、Cr、Moの一方または両方を含有し、Feを0.06%以下、Oを0.07%以下に制限し、Ni、V、Mn、Zr、Co、Ta、W、C、Nの1種または2種以上を合計で0.3%以下含有し、残部がTi及び不純物であり、金属組織がα相と第二相からなり、α相の平均結晶粒径が10〜50μmであり、個数密度が0.01個/μm2以上の測定領域の数が全測定領域の80%以上であるチタン合金板を採用する。【選択図】なし</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2021</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHAK8Qxx9PMM9VVw9PHxj1QI9nB1DdFRcPRzUXCN8HAMDQ5RCI4MDnH1VXD29w3w93P1CwlWcPMPUnAMDfH39Xfy9HHlYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBkaGBkYWJgbmjsZEKQIAcIcr2g</recordid><startdate>20210225</startdate><enddate>20210225</enddate><creator>TAKEBE HIDENORI</creator><creator>NISHIWAKI SOSUKE</creator><creator>KAWAKAMI AKIRA</creator><scope>EVB</scope></search><sort><creationdate>20210225</creationdate><title>TITANIUM ALLOY SHEET, AND EXHAUST SYSTEM COMPONENTS FOR AUTOMOBILE</title><author>TAKEBE HIDENORI ; NISHIWAKI SOSUKE ; KAWAKAMI AKIRA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2021028407A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2021</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>TAKEBE HIDENORI</creatorcontrib><creatorcontrib>NISHIWAKI SOSUKE</creatorcontrib><creatorcontrib>KAWAKAMI AKIRA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TAKEBE HIDENORI</au><au>NISHIWAKI SOSUKE</au><au>KAWAKAMI AKIRA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>TITANIUM ALLOY SHEET, AND EXHAUST SYSTEM COMPONENTS FOR AUTOMOBILE</title><date>2021-02-25</date><risdate>2021</risdate><abstract>To provide a titanium alloy sheet in which coarsening of crystal grains is suppressed under a high-temperature environment, and high-temperature strength is excellent.SOLUTION: A titanium alloy sheet contains Cu, Sn, Si, Nb and Al, contains one or both of Cr and Mo, Fe and O are limited to 0.06% or less and 0.07% or less respectively, contains one or two or more kinds of Ni, V, Mn, Zr, Co, Ta, W, C and N by 0.3% or less in total, balance is Ti and impurities, in which a metallic structure consists of an α phase and a second phase, the average crystal grain diameter of the α phase is 10 to 50 μm, and the number of measurement areas having the number density 0.01 piece/μm2 or more is 80% or more of all measurement areas.SELECTED DRAWING: None 【課題】高温環境下で結晶粒の粗大化が抑制され、高温強度に優れたチタン合金板を提供する。【解決手段】Cu、Sn、Si、Nb、Alを含有し、Cr、Moの一方または両方を含有し、Feを0.06%以下、Oを0.07%以下に制限し、Ni、V、Mn、Zr、Co、Ta、W、C、Nの1種または2種以上を合計で0.3%以下含有し、残部がTi及び不純物であり、金属組織がα相と第二相からなり、α相の平均結晶粒径が10〜50μmであり、個数密度が0.01個/μm2以上の測定領域の数が全測定領域の80%以上であるチタン合金板を採用する。【選択図】なし</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2021028407A
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title TITANIUM ALLOY SHEET, AND EXHAUST SYSTEM COMPONENTS FOR AUTOMOBILE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T18%3A07%3A01IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TAKEBE%20HIDENORI&rft.date=2021-02-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2021028407A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true