TITANIUM ALLOY SHEET, AND EXHAUST SYSTEM COMPONENTS FOR AUTOMOBILE
To provide a titanium alloy sheet in which coarsening of crystal grains is suppressed under a high-temperature environment, and high-temperature strength is excellent.SOLUTION: A titanium alloy sheet contains Cu, Sn, Si, Nb and Al, contains one or both of Cr and Mo, Fe and O are limited to 0.06% or...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide a titanium alloy sheet in which coarsening of crystal grains is suppressed under a high-temperature environment, and high-temperature strength is excellent.SOLUTION: A titanium alloy sheet contains Cu, Sn, Si, Nb and Al, contains one or both of Cr and Mo, Fe and O are limited to 0.06% or less and 0.07% or less respectively, contains one or two or more kinds of Ni, V, Mn, Zr, Co, Ta, W, C and N by 0.3% or less in total, balance is Ti and impurities, in which a metallic structure consists of an α phase and a second phase, the average crystal grain diameter of the α phase is 10 to 50 μm, and the number of measurement areas having the number density 0.01 piece/μm2 or more is 80% or more of all measurement areas.SELECTED DRAWING: None
【課題】高温環境下で結晶粒の粗大化が抑制され、高温強度に優れたチタン合金板を提供する。【解決手段】Cu、Sn、Si、Nb、Alを含有し、Cr、Moの一方または両方を含有し、Feを0.06%以下、Oを0.07%以下に制限し、Ni、V、Mn、Zr、Co、Ta、W、C、Nの1種または2種以上を合計で0.3%以下含有し、残部がTi及び不純物であり、金属組織がα相と第二相からなり、α相の平均結晶粒径が10〜50μmであり、個数密度が0.01個/μm2以上の測定領域の数が全測定領域の80%以上であるチタン合金板を採用する。【選択図】なし |
---|