DRAWN CONTAINER
To provide a drawn container that has superior drawing blow moldability, high container rigidity, and small container shrinkage after high-temperature sterilization processing.SOLUTION: A drawn container is formed of a propylene-based polymer composition (A) including: 0.5-45 mass% of a propylene-ba...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide a drawn container that has superior drawing blow moldability, high container rigidity, and small container shrinkage after high-temperature sterilization processing.SOLUTION: A drawn container is formed of a propylene-based polymer composition (A) including: 0.5-45 mass% of a propylene-based polymer (a1) of 10-12 dl/g in intrinsic viscosity [η] measured in a tetralin solvent at 135°C and 55-99.5 mass% of a propylene-based polymer (a2) of 0.5-3.5 dl/g in intrinsic viscosity [η] measured in the tetralin solution at 135°C (where a total mount of the propylene copolymer (a1) and propylene copolymer (a2) is 100 mass%).SELECTED DRAWING: None
【課題】延伸ブロー成形性に優れ、容器の剛性が高く、高温滅菌処理後の容器収縮が小さい延伸容器を提供する。【解決手段】135℃、テトラリン溶媒中で測定される極限粘度[η]が10〜12dl/gの範囲にあるプロピレン系重合体(a1)を0.5〜45質量%、および135℃、テトラリン溶媒中で測定される極限粘度[η]が0.5〜3.5dl/gの範囲にあるプロピレン系重合体(a2)を55〜99.5質量%〔ただし、プロピレン系重合体(a1)とプロピレン系重合体(a2)との合計量を100質量%とする。〕含むプロピレン系重合体組成物(A)からなる延伸容器。【選択図】なし |
---|