HIGH STRENGTH STEEL SHEET FOR HIGH HEAT INPUT WELDING

To provide a high strength steel sheet for high heat input welding based on new guidelines on component design.SOLUTION: A high strength steel sheet for high heat input welding contains, in mass%, C: 0.03-0.08%, Mn: 0.3-1.6%, Cu: 0.6-2.0%, Ni: 1.3-7.0%, Ti: 0.003-0.015%, Al: 0.03-0.10%, Cr: 0-1.1%,...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HONMA RYUICHI, FURUKAWA HIROTSUGU, URAKAWA TOMOKI, TAKAHIRA NOBUYUKI, SHINOHARA YASUHIRO, OTOMATSU YUKI, WATABE YOSHIYUKI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To provide a high strength steel sheet for high heat input welding based on new guidelines on component design.SOLUTION: A high strength steel sheet for high heat input welding contains, in mass%, C: 0.03-0.08%, Mn: 0.3-1.6%, Cu: 0.6-2.0%, Ni: 1.3-7.0%, Ti: 0.003-0.015%, Al: 0.03-0.10%, Cr: 0-1.1%, Mo: 0-1.0%, Nb: 0-0.03%, V: 0-0.10%, W: 0-1.0%, B: 0-0.0050%, Ca: 0-0.005%, Mg: 0-0.005%, REM: 0-0.005%, Zr: 0-0.005%, the balance being Fe and impurities, Ti/N of 3.0 or less, DI(inch) of 10.0-21.0, CeqWES of 0.500-0.700% or more, and CeqIIW of 0.650-0.890%.SELECTED DRAWING: None 【課題】新たな成分設計の指針に基づいて、大入熱溶接用高強度鋼板を提供する。【解決手段】本発明の大入熱溶接用高強度鋼板は、質量%で、C:0.03〜0.08%、Mn:0.3〜1.6%、Cu:0.6〜2.0%、Ni:1.3〜7.0%、Ti:0.003〜0.015%、Al:0.03〜0.10%、Cr:0〜1.1%、Mo:0〜1.0%、Nb:0〜0.03%、V:0〜0.10%、W:0〜1.0%、B:0〜0.0050%、Ca:0〜0.005%、Mg:0〜0.005%、REM:0〜0.005%、Zr:0〜0.005%、を含有し、残部がFe及び不純物からなり、Ti/Nが3.0以下であり、DI(inch)が10.0〜21.0であり、CeqWESが0.500〜0.700%以上であり、CeqIIWが0.650〜0.890%である。【選択図】なし