WHITE TONER AND METHOD FOR MANUFACTURING THE SAME
To provide a white toner excellent in bending resistance and a concealability.SOLUTION: A white toner comprises toner particles including a binder resin, an inorganic white pigment and a polyvalent metal salt compound. The inorganic white pigment has an acidic group on the surface; the content of th...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide a white toner excellent in bending resistance and a concealability.SOLUTION: A white toner comprises toner particles including a binder resin, an inorganic white pigment and a polyvalent metal salt compound. The inorganic white pigment has an acidic group on the surface; the content of the inorganic white pigment in the toner particles is 10-50 vol.%; the polyvalent metal salt compound is a specific compound; and the absolute value of a difference between the SP value (J/cm3)1/2 of the binder resin and the SP value (J/cm3)1/2 of the polyvalent metal salt compound is 0.0-6.0; When setting the content of the polyvalent metal salt compound in the toner particles to Wa [mass%], the amount of the polyvalent metal in the polyvalent metal salt compound to Ma [μmol/g], the content of the inorganic white pigment in the toner particles to Wp [mass%] and the surface acidic group amount of the inorganic white pigment to Ap [μmol/g], 0.1≤(Wa×Ma)/(Wp×Ap)≤2.0 is satisfied.SELECTED DRAWING: None
【課題】耐折り曲げ性及び隠蔽性に優れた白色トナー。【解決手段】結着樹脂、無機白色顔料、及び多価金属塩化合物を有するトナー粒子を含む白色トナーであって、該無機白色顔料は表面に酸性基を有し、該トナー粒子中の該無機白色顔料の含有量が、10体積%〜50体積%であり、該多価金属塩化合物は、特定の化合物であり、該結着樹脂のSP値(J/cm3)1/2と該多価金属塩化合物のSP値(J/cm3)1/2の差の絶対値が、0.0〜6.0であり、該トナー粒子中の該多価金属塩化合物の含有量をWa[質量%]とし、該多価金属塩化合物中の多価金属の量をMa[μmol/g]とし、該トナー粒子中の該無機白色顔料の含有量をWp[質量%]とし、該無機白色顔料の表面酸性基量をAp[μmol/g]としたとき、0.1≦(Wa×Ma)/(Wp×Ap)≦2.0を満たすことを特徴とする白色トナー。【選択図】なし |
---|