STAINLESS STEEL AND STAINLESS STEEL PIPE HAVING EXCELLENT ROUGE RESISTANCE, AND PURE STEAM ROUTE MEMBER

To provide a stainless steel having excellent rouge resistance.SOLUTION: A stainless steel has a composition that comprises C: 0.1 mass% or less, Si: 1.0 mass% or less, Mn: 2.0 mass% or less, P: 0.045 mass% or less, S: 0.03 mass% or less, Ni: 30 mass% or less, Cr: 16-35 mass%, Mo: 6.0 mass% or less,...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: IMAGAWA KAZUNARI, NOBUHARA YUTA, KAMATA MASAKATSU, NAKAGAMI SUSUMU, AKAJI HIROTSUGU, SAIDA TOMOAKI, NAKAJIMA TAKASHI, MATSUMOTO TOSHIJI, SEKIMUKAI KOTARO, HIROZUMI SHIRO
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To provide a stainless steel having excellent rouge resistance.SOLUTION: A stainless steel has a composition that comprises C: 0.1 mass% or less, Si: 1.0 mass% or less, Mn: 2.0 mass% or less, P: 0.045 mass% or less, S: 0.03 mass% or less, Ni: 30 mass% or less, Cr: 16-35 mass%, Mo: 6.0 mass% or less, Cu: 0.8 mass% or less, N: 0.3 mass% or less with the balance being Fe and inevitable impurities, and meets the relationship of formula (1) (where each element symbol denotes the content of each element). In the stainless steel, a passive coating has a Cr concentration of 40 atom% or more. Cr+0.5Mo≥19 (1).SELECTED DRAWING: None 【課題】耐ルージュ性に優れたステンレス鋼を提供する。【解決手段】C:0.1質量%以下、Si:1.0質量%以下、Mn:2.0質量%以下、P:0.045質量%以下、S:0.03質量%以下、Ni:30質量%以下、Cr:16〜35質量%、Mo:6.0質量%以下、Cu:0.8質量%以下、N:0.3質量%以下を含み、残部がFe及び不可避的不純物からなると共に、下記式(1)の関係(式中、各元素記号は、各元素の含有量を意味する)を満たす組成を有するステンレス鋼である。このステンレス鋼は、不働態皮膜中のCr濃度が40原子%以上である。Cr+0.5Mo≧19 (1)【選択図】なし