Cr-CONTAINING ELECTROSEAMED STEEL PIPE, AND MANUFACTURING METHOD THEREOF

To provide an electroseamed steel pipe excellent in corrosion resistance, and containing Cr over 3%.SOLUTION: In a Cr-containing electroseamed steel pipe containing Cr as much as 3.0-32.0 mass%, concerning Cr oxide defects existing on a welding surface, an evaluation length L, the maximum defective...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: WATANABE FUMINORI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To provide an electroseamed steel pipe excellent in corrosion resistance, and containing Cr over 3%.SOLUTION: In a Cr-containing electroseamed steel pipe containing Cr as much as 3.0-32.0 mass%, concerning Cr oxide defects existing on a welding surface, an evaluation length L, the maximum defective length Lin L, and a ratio Lbetween the evaluation length Land a total defect length (total of line lengths of exposed defects) satisfy following formulas (1), (2), and thereby corrosion resistance of a weld zone becomes equivalent to that of a parent metal: L[mm]≤0.1...(1) (100×L/L)[%]