METHOD FOR PRODUCING NEEDLE COKE
To provide the method for producing the needle coke with an improved physical property by chemical treatment of a tissue, wherein the needle coke is used as an aggregate of graphite electrode formation used for electrodes in an electric furnace industry.SOLUTION: The method for producing the needle...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide the method for producing the needle coke with an improved physical property by chemical treatment of a tissue, wherein the needle coke is used as an aggregate of graphite electrode formation used for electrodes in an electric furnace industry.SOLUTION: The method for producing the needle coke comprises: blowing again a calcined coke, that is produced by calcining raw coke produced by a delayed coking method at a temperature of 1200 to 1600°C with steam during a calcination process, converting selectively carbonaceous matter with an undeveloped needle-like tissue remaining in the calcined coke into hydrogen and carbon dioxide by a steam gasification reaction, removing the hydrogen and carbon dioxide, and leaving only a carbonaceous material with a developed needle-like tissue.SELECTED DRAWING: Figure 3
【課題】電炉工業での電極に用いられる黒鉛電極形成の骨材として用いられるニードルコークスの組織の化学的処理による物性改善【解決手段】ディレードコーキング法によって製造した生コークスを、1200〜1600℃の温度にてか焼することにより製造したか焼コークスを、再度か焼プロセス時に水蒸気を吹き込み、か焼コークスに残存している針状組織が発達していない炭素質を選択的に水蒸気ガス化反応により水素および二酸化炭素に変換、除去することにより、針状組織が発達した炭素質のみを残すニードルコークスの製造方法。【選択図】 図3 |
---|