ADHESIVE TAPE WITH BASE MATERIAL
To provide an adhesive tape with base material that strikes a balance between reworkability and adhesive strength.SOLUTION: An adhesive tape with base material has an addition reaction type silicone adhesive layer on a base film. After bonded to soda glass, it is allowed to stand for 30 minutes in a...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide an adhesive tape with base material that strikes a balance between reworkability and adhesive strength.SOLUTION: An adhesive tape with base material has an addition reaction type silicone adhesive layer on a base film. After bonded to soda glass, it is allowed to stand for 30 minutes in an environment of the temperature 23°C and the relative humidity 50%, showing an adhesion equal to or higher than 10 mN/25 mm in width and less than 300 mN/25 mm in width; or it is allowed to stand for 240 hours, showing an adhesion equal to or higher than 500 mN/25 mm or more in width and equal to or lower than 50000 mN/25 mm in width.SELECTED DRAWING: None
【課題】リワーク適性と接着強度が両立した基材付き粘着テープの提供。【解決手段】基材フィルム上に付加反応型シリコーン系粘着層を有する基材付き粘着テープであって、ソーダガラスに貼り合わせた後に23℃、相対湿度50%の環境中に30分静置した後の粘着力が10mN/25mm幅以上300mN/25mm幅未満であり、かつ、240時間静置した後の粘着力が500mN/25mm幅以上50000mN/25mm幅以下であることを特徴とする。【選択図】なし |
---|