METHOD FOR MANUFACTURING GLASS FILM

To preferably remove wrinkles generated in a glass film when cutting the glass film using peeling to accurately cut the glass film.SOLUTION: A conveyance step in a method for manufacturing a glass film G includes a wrinkle removal step of removing wrinkles of the glass film G by a wrinkle removal pa...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HASEGAWA YOSHINORI, MORI KOICHI, UEMURA HISAHIRO, MATSUMOTO NAOYUKI, AKIYAMA SHUJI, MORI HIROKI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To preferably remove wrinkles generated in a glass film when cutting the glass film using peeling to accurately cut the glass film.SOLUTION: A conveyance step in a method for manufacturing a glass film G includes a wrinkle removal step of removing wrinkles of the glass film G by a wrinkle removal part 20 arranged on the upstream side from a laser irradiation apparatus 25. A cutting step in the method for manufacturing the glass film G includes separating the glass film G by irradiating the glass film G with a laser beam L after removing the wrinkles Ge of the glass film G in the conveyance step and generating a thread-like peeled material Gg from a width direction end portion of the separated glass film G.SELECTED DRAWING: Figure 2 【課題】ピーリングを利用してガラスフィルムを切断する場合に、ガラスフィルムに生じ得る皺を好適に除去し、ガラスフィルムを精度良く切断する。【解決手段】ガラスフィルムGの製造方法における搬送工程は、レーザ照射装置25よりも上流側に配置される皺除去部20によりガラスフィルムGの皺を取り除く皺除去工程を備える。ガラスフィルムGの製造方法における切断工程は、搬送工程においてガラスフィルムGの皺Geを除去した後に、レーザ光LをガラスフィルムGに照射することによりガラスフィルムGを分離し、分離されたガラスフィルムGの幅方向端部から糸状剥離物Ggを発生させる。【選択図】図2