RADIATION DOSE MEASURING METHOD

PROBLEM TO BE SOLVED: To provide a radiation dose measuring method having high reproductivity and a glass for radiation detection.SOLUTION: A glass for radiation detection containing, by mol%, SiO+BO:0.1 to 30%, SiO:0 to 20%, BO:0 to 10%, PO:40 to 80%, AlO:1 to 30%, NaO:5 to 40%, AgO:0.01 to 2% is h...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAKAYAMA YOSHIHISA, IKEDA HIKARI, YAMAZAKI YOSHINORI, IWAO KATSU, NAKANE SHINGO
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a radiation dose measuring method having high reproductivity and a glass for radiation detection.SOLUTION: A glass for radiation detection containing, by mol%, SiO+BO:0.1 to 30%, SiO:0 to 20%, BO:0 to 10%, PO:40 to 80%, AlO:1 to 30%, NaO:5 to 40%, AgO:0.01 to 2% is heat treated in a temperature range of (glass transition point/4) to (glass transition point/2.5) to stabilize fluorescence intensity and then fluorescence intensity is measured. There is provided a glass for radiation detection further containing MgO:0 to 10% and ZnO:0 to 10%, and PO/(SiO+BO+AlO) with 1.2 or more by molar ratio.SELECTED DRAWING: None 【課題】高い再現性を有する放射線量測定方法及び放射線検出用ガラスの提供。【解決手段】モル%で、SiO2+B2O3:0.1〜30%、SiO2:0〜20%、B2O3:0〜10%、P2O5:40〜80%、Al2O3:1〜30%、Na2O:5〜40%、Ag2O:0.01〜2%を含有する放射線検出用ガラスを、(ガラス転移点/4)〜(ガラス転移点/2.5)の温度範囲で熱処理して蛍光強度を安定化した後に蛍光強度を測定する。更に、MgO:0〜10%、ZnO:0〜10%を含有し、モル比でP2O5/(SiO2+B2O3+Al2O3)1.2以上を含有することが好ましい放射線検出用ガラス。【選択図】なし