LAMINATION MOLDING METHOD
PROBLEM TO BE SOLVED: To provide a lamination molding method capable of preferably removing residual powder which is left in a path formed in a molded article.SOLUTION: Three-dimensional data for molding a molded article 50 is acquired (S10). Then, before producing the molded article 50 using a path...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a lamination molding method capable of preferably removing residual powder which is left in a path formed in a molded article.SOLUTION: Three-dimensional data for molding a molded article 50 is acquired (S10). Then, before producing the molded article 50 using a path model which simulates a path 60 using the three-dimensional data, on the basis of at least one of a flow rate and a flow velocity of a second fluid in the path model, removal property of the residual powder in the path 60 after the molded article 50 is produced using the three-dimensional data, is determined (S20). On the basis of the removal property determined in the step of S20, the three-dimensional data acquired in the step of the S10 is corrected (S30). Then, using the three-dimensional data corrected in the step of S30, the molded article 50 is produced by lamination molding (S40).SELECTED DRAWING: Figure 3
【課題】造形物の内部に形成された経路に残留する残留粉末を良好に除去することが可能な積層造形方法を提供する。【解決手段】造形物50を造形するための三次元データが取得される(S10)。三次元データを用いて経路60を模擬した経路モデルを用いて、造形物50を実際に製造する前に、経路モデルにおける第2の流体の流量及び流速の少なくとも一方に基づいて、三次元データを用いて造形物50が製造された後の経路60の残留粉末の除去性について判定される(S20)。S20の工程で判定された除去性に基づいて、S10の工程で取得された三次元データを修正する(S30)。S30の工程で修正された三次元データを用いて、積層造形によって造形物50を製造する(S40)。【選択図】図3 |
---|