TIRE PRODUCTION METHOD

PROBLEM TO BE SOLVED: To provide a tire production method capable of producing a tire excellent in heat durability while restraining deterioration of productivity.SOLUTION: A tire production method comprises a vulcanization process of vulcanizing a raw cover 10 in a mold 2 to obtain a tire. The vulc...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: OKAZAKI YURI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a tire production method capable of producing a tire excellent in heat durability while restraining deterioration of productivity.SOLUTION: A tire production method comprises a vulcanization process of vulcanizing a raw cover 10 in a mold 2 to obtain a tire. The vulcanization process includes a heating process of heating and pressurizing the raw cover 10 by filling a bladder 4 with steam in the closed mold 2, and a pressurizing process of heating and pressurizing the raw cover 10 by filling the bladder 4 with an inert gas in the closed mold 2. In the heating process, the inner pressure of the bladder 4 is 1,000 kPa or more but 2,000 kPa or less; the temperature of the steam is 180°C or higher but 220°C or lower; and a time Ti of the heating process is 5 minutes or less.SELECTED DRAWING: Figure 1 【課題】生産性の低下を抑制しつつ熱耐久性に優れるタイヤを製造しうる、タイヤの製造方法の提供。【解決手段】このタイヤの製造方法は、ローカバー10がモールド2内で加硫されてタイヤが得られる加硫工程を備えている。この加硫工程は、閉じられたモールド2内でブラダ4にスチームが充てんされてローカバー10が加熱及び加圧される加熱工程と、閉じられたモールド2内でブラダ4に不活性ガスが充てんされてローカバー10が加熱及び加圧される加圧工程とを備えている。この加熱工程において、ブラダ4の内圧は、1000kPa以上2000kPa以下である。スチームの温度は180℃以上220℃以下である。加熱工程の時間Tiは、5分以下である。【選択図】図1