COATING COMPOSITION, AND OPTICAL ARTICLE HAVING COAT LAYER MADE OF THE COATING COMPOSITION

PROBLEM TO BE SOLVED: To provide a coating composition forming a coat layer excellent in appearance, excoriation resistance, boiling adhesion and weather-resistant adhesion.SOLUTION: Provided is a coating composition comprising: inorganic oxide particles (A); a hydrolyzable group-containing organic...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: MORI RIKIHIRO
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a coating composition forming a coat layer excellent in appearance, excoriation resistance, boiling adhesion and weather-resistant adhesion.SOLUTION: Provided is a coating composition comprising: inorganic oxide particles (A); a hydrolyzable group-containing organic silicon compound (B); water or an acid aqueous solution (C); a hardening catalyst (D); an organic solvent (E); and aromatic alcohols (F). In the coating composition, the aromatic alcohols (F) are included in an amount of 3 to 100 pts.mass to 100 pts.mass of the total of the inorganic oxide particles (A) and the hydrolyzable group-containing organic silicon compound (B).SELECTED DRAWING: None 【課題】プラスチック製光学基材の表面に、外観、耐擦傷性、煮沸密着性、耐候密着性に優れたコート層を形成するコーティング組成物を提供する。【解決手段】無機酸化物微粒子(A)、加水分解性基含有有機ケイ素化合物(B)、水又は酸水溶液(C)、硬化触媒(D)、有機溶剤(E)、及び芳香族アルコール類(F)を含むコーティング組成物を提供する。該コーティング組成物において、前記芳香族アルコール類(F)が、前記無機酸化物微粒子(A)と前記加水分解性基含有有機ケイ素化合物(B)との合計量100質量部に対して、3〜100質量部の量で含むことが好ましい。【選択図】なし