REINFORCED BUILDING BLOCK MADE FROM AUTOCLAVE CURE AERATED CONCRETE (AAC)

PROBLEM TO BE SOLVED: To provide a building block which has excellent physical and mechanical characteristics compared to a technical level and provides improved heat resistance.SOLUTION: There are provided a reinforced building block made from autoclave cure aerated concrete (ACC) which has a reinf...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: VLADISLAV YAROSLAVSKIY, WLADIMIR RICHTER, ELENA TIMOFEEVA, DIRK FUCHSMANN, VOGEL MICHAEL
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a building block which has excellent physical and mechanical characteristics compared to a technical level and provides improved heat resistance.SOLUTION: There are provided a reinforced building block made from autoclave cure aerated concrete (ACC) which has a reinforcing bar formed from substantially at least one fibrous carrier A), a composition B) which is formed from at least one epoxy compound B1) and at least one diamine and/or polyamine B2) in a stoichiometric ratio of the epoxy compound B1) to the diamine and/or polyamine component B2) of 0.8:1 to 2:1, and is cured as a matrix material, and optionally further has a reinforcing bar formed of an auxiliary substance and an additive C); and a method for producing the same.SELECTED DRAWING: None 【課題】技術水準に比べて優れた物理的及び機械的特性を有する。改善された耐熱性を提供するために、建築ブロックで使用することができる。【解決手段】本発明は、オートクレーブ養生気泡コンクリート(ACC)製の強化された建築ブロックを対象とし、この強化された建築ブロックは、実質的に、少なくとも1種の繊維状担体A)、及び少なくとも1種のエポキシ化合物B1)及び少なくとも1種のジアミン及び/又はポリアミンB2)から、0.8:1〜2:1のエポキシ化合物B1)対ジアミン及び/又はポリアミン成分B2)の化学量論比で形成される、マトリックス材料としての硬化された組成物B)、及び任意でさらなる補助物質及び添加剤C)から形成される鉄筋を有し、また本発明は、その製造方法を対象とする。【選択図】なし