MANUFACTURING METHOD OF ANTIBACTERIAL AND DEODORANT FILM, ANTIBACTERIAL AND DEODORANT FILM AND PACKAGING MATERIAL
PROBLEM TO BE SOLVED: To provide a manufacturing method of an antibacterial and deodorant film, the antibacterial and deodorant film and packaging material capable of improving carrying capacity of antibacterial and deodorant material and capable of persistently retaining antibacterial and deodorant...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a manufacturing method of an antibacterial and deodorant film, the antibacterial and deodorant film and packaging material capable of improving carrying capacity of antibacterial and deodorant material and capable of persistently retaining antibacterial and deodorant performance.SOLUTION: A manufacturing method of an antibacterial and deodorant film includes: a process of applying first coating liquid 3' which contains foam microcapsule 2 and binder onto base material 1; a process of performing first drying processing to the first coating liquid 3' applied onto the base material 1 and foaming the foam microcapsule 2 to form a resin layer 3 which has a fine rugged structure produced by foaming on a surface thereof; a process of applying second coating liquid 6 which contains antibacterial and deodorant material 7 and does not contain binder onto a surface of the resin layer 3 and introducing the antibacterial and deodorant material 7 into a recessed part 5 of the rugged structure; and a process of performing second drying processing to the second coating liquid 6 applied onto the surface of the resin layer 3 and fixing the antibacterial and deodorant material 7 to an inner surface of the recessed part 5.SELECTED DRAWING: Figure 2
【課題】抗菌消臭材料の担持能力を高めることができ、抗菌消臭性能を持続性高く保持することが可能な抗菌消臭フィルムの製造方法、抗菌消臭フィルム及び包装材を提供する。【解決手段】発泡マイクロカプセル2とバインダーとを含む第1の塗工液3'を基材1上に塗工する工程と、基材1上に塗工された第1の塗工液3'に第1の乾燥処理を施して発泡マイクロカプセル2を発泡させ、発泡により生じた微細な凹凸構造を表面に有する樹脂層3を形成する工程と、抗菌消臭材料7を含み、かつバインダーを含まない第2の塗工液6を樹脂層3の表面に塗工して、抗菌消臭材料7を凹凸構造の凹部5内に導入する工程と、樹脂層3の表面に塗工された第2の塗工液6に第2の乾燥処理を施して、抗菌消臭材料7を凹部5の内面に固着させる工程と、を備える。【選択図】図2 |
---|