COATED MAGNETITE PARTICLE
PROBLEM TO BE SOLVED: To provide a magnetite particle having an octahedron shape and high dispersibility and high resistance.SOLUTION: A coated magnetite particle has a core particle of magnetite and a coating layer positioned with neighboring a surface of the core particle as an outermost layer. Th...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a magnetite particle having an octahedron shape and high dispersibility and high resistance.SOLUTION: A coated magnetite particle has a core particle of magnetite and a coating layer positioned with neighboring a surface of the core particle as an outermost layer. The coating layer positioned on each surface of an octahedron consist of oxide, the coating layer contains iron, silicon and aluminum and has a plurality of salients projecting from surfaces thereof. Average particle diameter of a primary particle measured by an electron microscope observation is 50 nm to 150 nm. Dust resistance is preferably 1.0×10Ω cm to 5.0×10Ω cm.SELECTED DRAWING: Figure 3
【課題】八面体の形状を有し、高分散、高抵抗であるマグネタイト粒子を提供すること。【解決手段】本発明の被覆マグネタイト粒子は、マグネタイトのコア粒子と、該コア粒子の表面に隣接して位置する最外層としての被覆層とを有する。被覆マグネタイト粒子は八面体の形状からなる。八面体における各面に位置する被覆層が酸化物からなり、該被覆層が鉄とケイ素とアルミニウムとを含み、かつ該被覆層はその表面から突出した複数の凸部を有する。電子顕微鏡観察によって測定された一次粒子の平均粒子径が50nm以上150nm以下である。圧粉抵抗が1.0×104Ω・cm以上5.0×106Ω・cm以下であることが好適である。【選択図】図3 |
---|