MANUFACTURING METHOD OF CEMENT CLINKER

PROBLEM TO BE SOLVED: To provide a manufacturing method of a cement clinker capable of reducing a burning temperature during manufacturing, capable of increasing waste using amount and reducing color tone change of the cement clinker even with increasing FeOcontent, compared to conventional cement c...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YOSHIMOTO SHINGO, SABAYASHI TAKASHI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a manufacturing method of a cement clinker capable of reducing a burning temperature during manufacturing, capable of increasing waste using amount and reducing color tone change of the cement clinker even with increasing FeOcontent, compared to conventional cement clinkers.SOLUTION: There is provided a manufacturing method of a cement clinker capable of reducing color tone change of the cement clinker even with increasing FeOcontent by blending a raw material so that total amount of CA and CAF calculated by a Bogue equation is 22% or more, CS amount is 60% or more and iron modulus (I.M) of 1.3 or less and using titanium slag as an FeOsource in the blending raw material. There is provided a manufacturing method of the cement clinker preferably by adjusting a raw material with further CAF amount of 15% or more.SELECTED DRAWING: None 【課題】従来のセメントクリンカーに比べ、製造する際の焼成温度を低減することが可能であり、廃棄物使用量を増やすことが可能であり、Fe2O3含有量が増加してもセメントクリンカーの色調変化を低減できるセメントクリンカーの製造方法を提供。【解決手段】ボーグ式により算出されるC3AおよびC4AFの合計量が22%以上、C3S量が60%以上、かつ鉄率(I.M.)が1.3以下となるように原料を調合し、該調合原料におけるFe2O3源としてチタン鉱滓を使用することで、Fe2O3含有量が増加してもセメントクリンカーの色調変化を低減できるセメントクリンカーの製造方法。更にC4AF量が15%以上となる様に原料を調整することが好ましいセメントクリンカーの製造方法。【選択図】なし