MANUFACTURING METHOD OF BARRIER FILM AND PLASMA CVD APPARATUS

PROBLEM TO BE SOLVED: To provide a technology to increase a film deposition rate without accompanying a large scale change of a system configuration, in a film deposition by a plasma CVD method.SOLUTION: A manufacturing method of a barrier film according to the invention forms a barrier layer contai...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KAWAKAMI NOBUYUKI, OKIMOTO TADAO, JIKO NORIHIRO
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a technology to increase a film deposition rate without accompanying a large scale change of a system configuration, in a film deposition by a plasma CVD method.SOLUTION: A manufacturing method of a barrier film according to the invention forms a barrier layer containing silicon, carbon and oxygen on one or both sides of a substrate film by a plasma CVD method. Gas for forming the barrier layer of the plasma CVD method contains organic silicon compound gas and oxidizing gas. In a chemical equation when the organic silicon compound is completely oxidized, (A-B)/B is 6.75 or less, where A is a total molecular number of a molecular formed by an oxidation reaction, and B is the number of silicon atoms in the organic silicon compound.SELECTED DRAWING: Figure 1 【課題】プラズマCVD法でのバリア層の成膜において、装置構成の大がかりな変更を伴うことなく成膜速度を増加できる技術を提供する。【解決手段】本発明は、プラズマCVD法によって、基材フィルムの片面もしくは両面にケイ素、炭素及び酸素を含むバリア層を形成するバリアフィルムの製造方法であって、前記プラズマCVD法のバリア層形成用ガスは、有機ケイ素化合物ガス及び酸化性ガスを含有し、前記有機ケイ素化合物を完全に酸化した場合の化学反応式において、酸化反応によって生成する分子の全分子数をA、前記有機ケイ素化合物中のケイ素の原子数をBとするとき、(A−B)/Bの値が6.75以下であることを特徴とするバリアフィルムの製造方法である。【選択図】図1