EXPANDED SHEET AND METHOD FOR PRODUCING THE SAME

PROBLEM TO BE SOLVED: To provide an expanded sheet that exhibits a moderate tackiness, a good wet skid resistance, an abrasion resistance and an impact resistance, as well as to provide a method for producing an expanded sheet that can improve the workability.SOLUTION: Provided is: an expanded sheet...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: ISOMURA HITOSHI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ISOMURA HITOSHI
description PROBLEM TO BE SOLVED: To provide an expanded sheet that exhibits a moderate tackiness, a good wet skid resistance, an abrasion resistance and an impact resistance, as well as to provide a method for producing an expanded sheet that can improve the workability.SOLUTION: Provided is: an expanded sheet obtained by forming a raw-material containing (A) a hydrogenated butadiene-based polymer having a number average molecular weight of 2,000 to 3,500, (B) a thermoplastic polymer other than (A) component, and (C) a blowing agent, into sheet-shape, and in which the hydrogenated butadiene-based polymer (A) is heated to 180°C to 200°C and mixed into the raw-material; and an expanded sheet in which the hydrogenated butadiene-based polymer (A) contains 1,2-vinyl bond by 50% or more, both ends comprises a hydroxyl group, and the incorporation amount is 2 to 10 weight% relative to the raw-material total amount.SELECTED DRAWING: Figure 1 【課題】適度な粘着性、良好な湿潤滑り抵抗、耐摩耗性および耐衝撃性を発揮する発泡シート、ならびに作業性を向上することのできる発泡シートの製造方法の提供。【解決手段】(A)数平均分子量が2,000〜3,500の水素化ブタジエン系重合体と、(B)(A)成分以外の熱可塑性重合体と、(C)発泡剤と、を含む原料をシート状に成形する発泡シートであって、水素化ブタジエン系重合体(A)を180℃〜200℃に加熱させて前記原料に混合する発泡シート。水素化ブタジエン系重合体(A)は、1,2−ビニル結合を50%以上有し、両末端が水酸基を有し、その配合量が原料全量に対し2〜10重量%である、発泡シート。【選択図】図1
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2016113554A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2016113554A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2016113554A3</originalsourceid><addsrcrecordid>eNrjZDBwjQhw9HNxdVEI9nB1DVEAshV8XUM8_F0U3PyDFAKC_F1CnT393BVCPFwVgh19XXkYWNMSc4pTeaE0N4OSm2uIs4duakF-fGpxQWJyal5qSbxXgJGBoZmhobGpqYmjMVGKAE7oJlI</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>EXPANDED SHEET AND METHOD FOR PRODUCING THE SAME</title><source>esp@cenet</source><creator>ISOMURA HITOSHI</creator><creatorcontrib>ISOMURA HITOSHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide an expanded sheet that exhibits a moderate tackiness, a good wet skid resistance, an abrasion resistance and an impact resistance, as well as to provide a method for producing an expanded sheet that can improve the workability.SOLUTION: Provided is: an expanded sheet obtained by forming a raw-material containing (A) a hydrogenated butadiene-based polymer having a number average molecular weight of 2,000 to 3,500, (B) a thermoplastic polymer other than (A) component, and (C) a blowing agent, into sheet-shape, and in which the hydrogenated butadiene-based polymer (A) is heated to 180°C to 200°C and mixed into the raw-material; and an expanded sheet in which the hydrogenated butadiene-based polymer (A) contains 1,2-vinyl bond by 50% or more, both ends comprises a hydroxyl group, and the incorporation amount is 2 to 10 weight% relative to the raw-material total amount.SELECTED DRAWING: Figure 1 【課題】適度な粘着性、良好な湿潤滑り抵抗、耐摩耗性および耐衝撃性を発揮する発泡シート、ならびに作業性を向上することのできる発泡シートの製造方法の提供。【解決手段】(A)数平均分子量が2,000〜3,500の水素化ブタジエン系重合体と、(B)(A)成分以外の熱可塑性重合体と、(C)発泡剤と、を含む原料をシート状に成形する発泡シートであって、水素化ブタジエン系重合体(A)を180℃〜200℃に加熱させて前記原料に混合する発泡シート。水素化ブタジエン系重合体(A)は、1,2−ビニル結合を50%以上有し、両末端が水酸基を有し、その配合量が原料全量に対し2〜10重量%である、発泡シート。【選択図】図1</description><language>eng ; jpn</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; GENERAL PROCESSES OF COMPOUNDING ; LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; WORKING-UP</subject><creationdate>2016</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160623&amp;DB=EPODOC&amp;CC=JP&amp;NR=2016113554A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20160623&amp;DB=EPODOC&amp;CC=JP&amp;NR=2016113554A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ISOMURA HITOSHI</creatorcontrib><title>EXPANDED SHEET AND METHOD FOR PRODUCING THE SAME</title><description>PROBLEM TO BE SOLVED: To provide an expanded sheet that exhibits a moderate tackiness, a good wet skid resistance, an abrasion resistance and an impact resistance, as well as to provide a method for producing an expanded sheet that can improve the workability.SOLUTION: Provided is: an expanded sheet obtained by forming a raw-material containing (A) a hydrogenated butadiene-based polymer having a number average molecular weight of 2,000 to 3,500, (B) a thermoplastic polymer other than (A) component, and (C) a blowing agent, into sheet-shape, and in which the hydrogenated butadiene-based polymer (A) is heated to 180°C to 200°C and mixed into the raw-material; and an expanded sheet in which the hydrogenated butadiene-based polymer (A) contains 1,2-vinyl bond by 50% or more, both ends comprises a hydroxyl group, and the incorporation amount is 2 to 10 weight% relative to the raw-material total amount.SELECTED DRAWING: Figure 1 【課題】適度な粘着性、良好な湿潤滑り抵抗、耐摩耗性および耐衝撃性を発揮する発泡シート、ならびに作業性を向上することのできる発泡シートの製造方法の提供。【解決手段】(A)数平均分子量が2,000〜3,500の水素化ブタジエン系重合体と、(B)(A)成分以外の熱可塑性重合体と、(C)発泡剤と、を含む原料をシート状に成形する発泡シートであって、水素化ブタジエン系重合体(A)を180℃〜200℃に加熱させて前記原料に混合する発泡シート。水素化ブタジエン系重合体(A)は、1,2−ビニル結合を50%以上有し、両末端が水酸基を有し、その配合量が原料全量に対し2〜10重量%である、発泡シート。【選択図】図1</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2016</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDBwjQhw9HNxdVEI9nB1DVEAshV8XUM8_F0U3PyDFAKC_F1CnT393BVCPFwVgh19XXkYWNMSc4pTeaE0N4OSm2uIs4duakF-fGpxQWJyal5qSbxXgJGBoZmhobGpqYmjMVGKAE7oJlI</recordid><startdate>20160623</startdate><enddate>20160623</enddate><creator>ISOMURA HITOSHI</creator><scope>EVB</scope></search><sort><creationdate>20160623</creationdate><title>EXPANDED SHEET AND METHOD FOR PRODUCING THE SAME</title><author>ISOMURA HITOSHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2016113554A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2016</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>ISOMURA HITOSHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ISOMURA HITOSHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>EXPANDED SHEET AND METHOD FOR PRODUCING THE SAME</title><date>2016-06-23</date><risdate>2016</risdate><abstract>PROBLEM TO BE SOLVED: To provide an expanded sheet that exhibits a moderate tackiness, a good wet skid resistance, an abrasion resistance and an impact resistance, as well as to provide a method for producing an expanded sheet that can improve the workability.SOLUTION: Provided is: an expanded sheet obtained by forming a raw-material containing (A) a hydrogenated butadiene-based polymer having a number average molecular weight of 2,000 to 3,500, (B) a thermoplastic polymer other than (A) component, and (C) a blowing agent, into sheet-shape, and in which the hydrogenated butadiene-based polymer (A) is heated to 180°C to 200°C and mixed into the raw-material; and an expanded sheet in which the hydrogenated butadiene-based polymer (A) contains 1,2-vinyl bond by 50% or more, both ends comprises a hydroxyl group, and the incorporation amount is 2 to 10 weight% relative to the raw-material total amount.SELECTED DRAWING: Figure 1 【課題】適度な粘着性、良好な湿潤滑り抵抗、耐摩耗性および耐衝撃性を発揮する発泡シート、ならびに作業性を向上することのできる発泡シートの製造方法の提供。【解決手段】(A)数平均分子量が2,000〜3,500の水素化ブタジエン系重合体と、(B)(A)成分以外の熱可塑性重合体と、(C)発泡剤と、を含む原料をシート状に成形する発泡シートであって、水素化ブタジエン系重合体(A)を180℃〜200℃に加熱させて前記原料に混合する発泡シート。水素化ブタジエン系重合体(A)は、1,2−ビニル結合を50%以上有し、両末端が水酸基を有し、その配合量が原料全量に対し2〜10重量%である、発泡シート。【選択図】図1</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; jpn
recordid cdi_epo_espacenet_JP2016113554A
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
CHEMISTRY
COMPOSITIONS BASED THEREON
GENERAL PROCESSES OF COMPOUNDING
LAYERED PRODUCTS
LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
PERFORMING OPERATIONS
THEIR PREPARATION OR CHEMICAL WORKING-UP
TRANSPORTING
WORKING-UP
title EXPANDED SHEET AND METHOD FOR PRODUCING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-11T05%3A52%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ISOMURA%20HITOSHI&rft.date=2016-06-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2016113554A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true