AGGREGATE AND PRODUCTION METHOD THEREOF

PROBLEM TO BE SOLVED: To produce aggregate from coal ash.SOLUTION: Coal ash 11 and cement 40 put in mixing treatment cabinets 2, 64 are mixed by mixing means 4B while misty water 42 is put into it, so that granulated aggregate components can be produced. Thus, the coal ash 11, which is combustion wa...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANAGAWA SHINJI, MIYAMOTO MIYO, GIORGIO FERRARI, MIYAMOTO MITSUYA, ALBERTO FERRARI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To produce aggregate from coal ash.SOLUTION: Coal ash 11 and cement 40 put in mixing treatment cabinets 2, 64 are mixed by mixing means 4B while misty water 42 is put into it, so that granulated aggregate components can be produced. Thus, the coal ash 11, which is combustion waste from a thermal power plant basically, can be utilized effectively as raw material for the construction of facilities. 【課題】石炭灰から骨材を生成する。【解決手段】練り混ぜ処理筐体2、64に入れた石炭灰11及びセメント40を練り混ぜ手段4Bによって練り混ぜながら霧状水42を入れることにより、粒状化した骨材成分を生成できるようにしたことにより、本来は火力発電所からの燃焼廃棄材である石炭灰11を設備構築用原材料として有効に活用することができる。【選択図】図4