RUBBER COMPOSITION FOR VIBRATION-PROOF RUBBER AND VIBRATION-PROOF RUBBER

PROBLEM TO BE SOLVED: To provide a rubber composition for vibration-proof rubber and a vibration-proof rubber capable of achieving both high durability and low dynamic magnification.SOLUTION: There is provided a rubber composition for vibration-proof rubber which comprises 2 to 10 pts.wt. of composi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TOKUNAGA SHUICHI, YUKIMOTO NAOTO
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a rubber composition for vibration-proof rubber and a vibration-proof rubber capable of achieving both high durability and low dynamic magnification.SOLUTION: There is provided a rubber composition for vibration-proof rubber which comprises 2 to 10 pts.wt. of composite zinc white based on 100 pts.wt. of a rubber component containing 60 to 95 pts.wt. of at least one selected from the group consisting of a natural rubber and a polyisoprene rubber and 5 to 30 pts.wt. of a styrene-butadiene rubber. The composite zinc white is obtained by coating a core such as CaCohaving a core diameter as small as possible with zinc oxide and has a nitrogen adsorption specific surface area of 15 to 110 m/g, a DBP oil absorption of 50 to 100 ml/100 g and a zinc oxide concentration of 38 to 64 wt.%. 【課題】高耐久性および低動倍率性の両立が可能な防振ゴム用ゴム組成物および防振ゴムを提供すること。【解決手段】天然ゴムおよびポリイソプレンゴムからなる群より選択される少なくとも1種60〜95重量部ならびにスチレンブタジエンゴム5〜30重量部を含むゴム成分100重量部に対し、複合亜鉛華を2〜10重量部含有し、該複合亜鉛華が、できるだけ小さなcore径を有するCaCo3などのcoreに亜鉛華を被覆したものであって、窒素吸着比表面積が15〜110m2/g、DBP吸油量が50〜100ml/100g、かつ亜鉛華濃度が38〜64重量%である防振ゴム用ゴム組成物。【選択図】 なし