FIXED ABRASIVE GRAIN WIRE AND WIRE PROCESSING METHOD

PROBLEM TO BE SOLVED: To provide an abrasive grain wire capable of improving sharpness and reducing a processing cost when an alloy containing iron of 45% or more such as an alnico alloy, a ferritic alloy, a samarium-cobalt alloy, a neodymium alloy and the like is cut and to provide a wire processin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAWARA SHINJI, TOGE NAOKI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide an abrasive grain wire capable of improving sharpness and reducing a processing cost when an alloy containing iron of 45% or more such as an alnico alloy, a ferritic alloy, a samarium-cobalt alloy, a neodymium alloy and the like is cut and to provide a wire processing method using the same.SOLUTION: In an abrasive grain wire 2 using for cutting an alloy containing iron of 45% or more,: abrasive grains fixed on a wire 6 include both of diamond abrasive grains 7 and CBN abrasive grains 8; and an including ratio of the diamond abrasive grains 7 to the CBN abrasive grains 8 is 20:80-70:30. 【課題】アルニコ合金、フェライト合金、サマコバ合金やネオジム合金等の鉄を45%以上含有する合金の切断に際して、切味の向上および加工コストの低減を可能にした固定砥粒ワイヤーおよびこれを用いたワイヤー加工方法の提供。【解決手段】鉄を45%以上含有する合金の切断に用いられる固定砥粒ワイヤー2であって、ワイヤー6上に固定される砥粒が、ダイヤモンド砥粒7およびCBN砥粒8の両方を含み、ダイヤモンド砥粒7とCBN砥粒8との含有比率を20:80〜70:30とした。【選択図】図2