METHOD FOR PRODUCING HEAT-RESISTANT ALUMINUM HYDROXIDE
PROBLEM TO BE SOLVED: To provide a method for producing aluminum hydroxide capable of withstanding the working temperature of a resin by applying high heat history while suppressing the defect and dehydration of its surface.SOLUTION: Provided is a method for producing heat-resistant aluminum hydroxi...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a method for producing aluminum hydroxide capable of withstanding the working temperature of a resin by applying high heat history while suppressing the defect and dehydration of its surface.SOLUTION: Provided is a method for producing heat-resistant aluminum hydroxide including heating treatment to gibbsite type aluminum hydroxide at a temperature of 180 to 300°C under the pressure of an atmospheric pressure or higher to 0.3 MPa or lower in an atmosphere satisfying a water vapor mol fraction of 0.03 to 1. |
---|