CONTINUOUS NORMAL PRESSURE VULCANIZATION METHOD
PROBLEM TO BE SOLVED: To provide a continuous normal pressure vulcanization method with which an unvulcanized rubber product is continuously vulcanized with vulcanization speed nearly equal to extrusion speed, while retaining the shape of the product even when the unvulcanized rubber product to be e...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a continuous normal pressure vulcanization method with which an unvulcanized rubber product is continuously vulcanized with vulcanization speed nearly equal to extrusion speed, while retaining the shape of the product even when the unvulcanized rubber product to be extrusion molded is long and has a large cross-sectional shape.SOLUTION: An unvulcanized rubber product D to be molded with continuous extrusion is sent to, and immersed in, a liquid vulcanization tank 3 in which a liquid heat medium 5, consisting of one liquid or a plurality of liquids with specific gravity less than that of the unvulcanized rubber product, is heated and stored, and vulcanized under normal pressure. The unvulcanized rubber product is continuously vulcanized by maintaining an immersed state in the liquid heat medium 5 without being floated with buoyancy, and uniformly heating the product, while retaining the shape, in accordance with extrusion speed under normal pressure. |
---|