POLYMERIZED CURED PRODUCT AND METHOD FOR PRODUCING THE SAME

PROBLEM TO BE SOLVED: To provide a raw material with high storage stability for producing polythioether which has excellent mechanical performance (high bending strength, high bending fracture strain, and high glass transition temperature) in addition to excellent optical performance (high refractiv...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HIRAKAWA TAKAFUMI, MORIGAMI ATSUSHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HIRAKAWA TAKAFUMI
MORIGAMI ATSUSHI
description PROBLEM TO BE SOLVED: To provide a raw material with high storage stability for producing polythioether which has excellent mechanical performance (high bending strength, high bending fracture strain, and high glass transition temperature) in addition to excellent optical performance (high refractive index, high Abbe number, and high transmittance) and exhibits excellent properties as an optical material.SOLUTION: Provided is polythiourethane polythiol prepared by reacting a polythiol compound with a polyiso(thio)cyanate compound without including an episulfide compound. The polythiourethane polythiol is a liquid at 25°C, and has a repeating unit represented by the general formula (1). The polythiourethane polythiol provides a cured product by reaction of a terminal mercapto group.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2014077135A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2014077135A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2014077135A3</originalsourceid><addsrcrecordid>eNrjZLAO8PeJ9HUN8oxydVFwDg0CkgFB_i6hziEKjn4uCr6uIR7-Lgpu_kFQYU8_d4UQD1eFYEdfVx4G1rTEnOJUXijNzaDk5hri7KGbWpAfn1pckJicmpdaEu8VYGRgaGJgbm5obOpoTJQiAC8RKac</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>POLYMERIZED CURED PRODUCT AND METHOD FOR PRODUCING THE SAME</title><source>esp@cenet</source><creator>HIRAKAWA TAKAFUMI ; MORIGAMI ATSUSHI</creator><creatorcontrib>HIRAKAWA TAKAFUMI ; MORIGAMI ATSUSHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a raw material with high storage stability for producing polythioether which has excellent mechanical performance (high bending strength, high bending fracture strain, and high glass transition temperature) in addition to excellent optical performance (high refractive index, high Abbe number, and high transmittance) and exhibits excellent properties as an optical material.SOLUTION: Provided is polythiourethane polythiol prepared by reacting a polythiol compound with a polyiso(thio)cyanate compound without including an episulfide compound. The polythiourethane polythiol is a liquid at 25°C, and has a repeating unit represented by the general formula (1). The polythiourethane polythiol provides a cured product by reaction of a terminal mercapto group.</description><language>eng</language><subject>ACYCLIC OR CARBOCYCLIC COMPOUNDS ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; ORGANIC CHEMISTRY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2014</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20140501&amp;DB=EPODOC&amp;CC=JP&amp;NR=2014077135A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20140501&amp;DB=EPODOC&amp;CC=JP&amp;NR=2014077135A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HIRAKAWA TAKAFUMI</creatorcontrib><creatorcontrib>MORIGAMI ATSUSHI</creatorcontrib><title>POLYMERIZED CURED PRODUCT AND METHOD FOR PRODUCING THE SAME</title><description>PROBLEM TO BE SOLVED: To provide a raw material with high storage stability for producing polythioether which has excellent mechanical performance (high bending strength, high bending fracture strain, and high glass transition temperature) in addition to excellent optical performance (high refractive index, high Abbe number, and high transmittance) and exhibits excellent properties as an optical material.SOLUTION: Provided is polythiourethane polythiol prepared by reacting a polythiol compound with a polyiso(thio)cyanate compound without including an episulfide compound. The polythiourethane polythiol is a liquid at 25°C, and has a repeating unit represented by the general formula (1). The polythiourethane polythiol provides a cured product by reaction of a terminal mercapto group.</description><subject>ACYCLIC OR CARBOCYCLIC COMPOUNDS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC CHEMISTRY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2014</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAO8PeJ9HUN8oxydVFwDg0CkgFB_i6hziEKjn4uCr6uIR7-Lgpu_kFQYU8_d4UQD1eFYEdfVx4G1rTEnOJUXijNzaDk5hri7KGbWpAfn1pckJicmpdaEu8VYGRgaGJgbm5obOpoTJQiAC8RKac</recordid><startdate>20140501</startdate><enddate>20140501</enddate><creator>HIRAKAWA TAKAFUMI</creator><creator>MORIGAMI ATSUSHI</creator><scope>EVB</scope></search><sort><creationdate>20140501</creationdate><title>POLYMERIZED CURED PRODUCT AND METHOD FOR PRODUCING THE SAME</title><author>HIRAKAWA TAKAFUMI ; MORIGAMI ATSUSHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2014077135A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2014</creationdate><topic>ACYCLIC OR CARBOCYCLIC COMPOUNDS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC CHEMISTRY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>HIRAKAWA TAKAFUMI</creatorcontrib><creatorcontrib>MORIGAMI ATSUSHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HIRAKAWA TAKAFUMI</au><au>MORIGAMI ATSUSHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>POLYMERIZED CURED PRODUCT AND METHOD FOR PRODUCING THE SAME</title><date>2014-05-01</date><risdate>2014</risdate><abstract>PROBLEM TO BE SOLVED: To provide a raw material with high storage stability for producing polythioether which has excellent mechanical performance (high bending strength, high bending fracture strain, and high glass transition temperature) in addition to excellent optical performance (high refractive index, high Abbe number, and high transmittance) and exhibits excellent properties as an optical material.SOLUTION: Provided is polythiourethane polythiol prepared by reacting a polythiol compound with a polyiso(thio)cyanate compound without including an episulfide compound. The polythiourethane polythiol is a liquid at 25°C, and has a repeating unit represented by the general formula (1). The polythiourethane polythiol provides a cured product by reaction of a terminal mercapto group.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2014077135A
source esp@cenet
subjects ACYCLIC OR CARBOCYCLIC COMPOUNDS
CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
ORGANIC CHEMISTRY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title POLYMERIZED CURED PRODUCT AND METHOD FOR PRODUCING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-31T13%3A56%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HIRAKAWA%20TAKAFUMI&rft.date=2014-05-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2014077135A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true