PEEP-PREVENTING FILM AND METHOD FOR MANUFACTURING THE SAME
PROBLEM TO BE SOLVED: To eliminate a defective wall part in a method for manufacturing a peep-preventing film configured to include a transparent observation part, an opaque wall part formed between the observation part, and a pair of substrates sandwiching the observation part and the wall part.SOL...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | FUJIWARA SHIGERU KITAHARA HIDETOSHI KOKUBO MITSUNORI MUROFUSE ISAMU OMAGARI HIROAKI |
description | PROBLEM TO BE SOLVED: To eliminate a defective wall part in a method for manufacturing a peep-preventing film configured to include a transparent observation part, an opaque wall part formed between the observation part, and a pair of substrates sandwiching the observation part and the wall part.SOLUTION: A method for manufacturing a peep-preventing film includes: an observation part producing step of producing an observation part 5 on one surface of a first substrate 3 having a light-permeation material in a thickness direction; a second substrate installation step of providing a second substrate 9 having the light-permeation material so that one surface of the second substrate 9 in the thickness direction faces the observation part 5 and the second substrate 9 is inserted in the observation part 5 in cooperation with the first substrate 3; a molded article installation step of providing a molded article 25 in a gap between the observation parts 5; and a wall part producing step of producing an opaque wall part 7 by curing the molded article 25 at the center 13 of the substrates 3, 9. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2013233696A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2013233696A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2013233696A3</originalsourceid><addsrcrecordid>eNrjZLAKcHUN0A0Icg1z9Qvx9HNXcPP08VVw9HNR8HUN8fB3UXDzD1LwdfQLdXN0DgkNAqkI8XBVCHb0deVhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhsZGxsZmlmaOxkQpAgD1OilS</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PEEP-PREVENTING FILM AND METHOD FOR MANUFACTURING THE SAME</title><source>esp@cenet</source><creator>FUJIWARA SHIGERU ; KITAHARA HIDETOSHI ; KOKUBO MITSUNORI ; MUROFUSE ISAMU ; OMAGARI HIROAKI</creator><creatorcontrib>FUJIWARA SHIGERU ; KITAHARA HIDETOSHI ; KOKUBO MITSUNORI ; MUROFUSE ISAMU ; OMAGARI HIROAKI</creatorcontrib><description>PROBLEM TO BE SOLVED: To eliminate a defective wall part in a method for manufacturing a peep-preventing film configured to include a transparent observation part, an opaque wall part formed between the observation part, and a pair of substrates sandwiching the observation part and the wall part.SOLUTION: A method for manufacturing a peep-preventing film includes: an observation part producing step of producing an observation part 5 on one surface of a first substrate 3 having a light-permeation material in a thickness direction; a second substrate installation step of providing a second substrate 9 having the light-permeation material so that one surface of the second substrate 9 in the thickness direction faces the observation part 5 and the second substrate 9 is inserted in the observation part 5 in cooperation with the first substrate 3; a molded article installation step of providing a molded article 25 in a gap between the observation parts 5; and a wall part producing step of producing an opaque wall part 7 by curing the molded article 25 at the center 13 of the substrates 3, 9.</description><language>eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; PERFORMING OPERATIONS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20131121&DB=EPODOC&CC=JP&NR=2013233696A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20131121&DB=EPODOC&CC=JP&NR=2013233696A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>FUJIWARA SHIGERU</creatorcontrib><creatorcontrib>KITAHARA HIDETOSHI</creatorcontrib><creatorcontrib>KOKUBO MITSUNORI</creatorcontrib><creatorcontrib>MUROFUSE ISAMU</creatorcontrib><creatorcontrib>OMAGARI HIROAKI</creatorcontrib><title>PEEP-PREVENTING FILM AND METHOD FOR MANUFACTURING THE SAME</title><description>PROBLEM TO BE SOLVED: To eliminate a defective wall part in a method for manufacturing a peep-preventing film configured to include a transparent observation part, an opaque wall part formed between the observation part, and a pair of substrates sandwiching the observation part and the wall part.SOLUTION: A method for manufacturing a peep-preventing film includes: an observation part producing step of producing an observation part 5 on one surface of a first substrate 3 having a light-permeation material in a thickness direction; a second substrate installation step of providing a second substrate 9 having the light-permeation material so that one surface of the second substrate 9 in the thickness direction faces the observation part 5 and the second substrate 9 is inserted in the observation part 5 in cooperation with the first substrate 3; a molded article installation step of providing a molded article 25 in a gap between the observation parts 5; and a wall part producing step of producing an opaque wall part 7 by curing the molded article 25 at the center 13 of the substrates 3, 9.</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>PERFORMING OPERATIONS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAKcHUN0A0Icg1z9Qvx9HNXcPP08VVw9HNR8HUN8fB3UXDzD1LwdfQLdXN0DgkNAqkI8XBVCHb0deVhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhsZGxsZmlmaOxkQpAgD1OilS</recordid><startdate>20131121</startdate><enddate>20131121</enddate><creator>FUJIWARA SHIGERU</creator><creator>KITAHARA HIDETOSHI</creator><creator>KOKUBO MITSUNORI</creator><creator>MUROFUSE ISAMU</creator><creator>OMAGARI HIROAKI</creator><scope>EVB</scope></search><sort><creationdate>20131121</creationdate><title>PEEP-PREVENTING FILM AND METHOD FOR MANUFACTURING THE SAME</title><author>FUJIWARA SHIGERU ; KITAHARA HIDETOSHI ; KOKUBO MITSUNORI ; MUROFUSE ISAMU ; OMAGARI HIROAKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2013233696A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2013</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>PERFORMING OPERATIONS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>FUJIWARA SHIGERU</creatorcontrib><creatorcontrib>KITAHARA HIDETOSHI</creatorcontrib><creatorcontrib>KOKUBO MITSUNORI</creatorcontrib><creatorcontrib>MUROFUSE ISAMU</creatorcontrib><creatorcontrib>OMAGARI HIROAKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>FUJIWARA SHIGERU</au><au>KITAHARA HIDETOSHI</au><au>KOKUBO MITSUNORI</au><au>MUROFUSE ISAMU</au><au>OMAGARI HIROAKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PEEP-PREVENTING FILM AND METHOD FOR MANUFACTURING THE SAME</title><date>2013-11-21</date><risdate>2013</risdate><abstract>PROBLEM TO BE SOLVED: To eliminate a defective wall part in a method for manufacturing a peep-preventing film configured to include a transparent observation part, an opaque wall part formed between the observation part, and a pair of substrates sandwiching the observation part and the wall part.SOLUTION: A method for manufacturing a peep-preventing film includes: an observation part producing step of producing an observation part 5 on one surface of a first substrate 3 having a light-permeation material in a thickness direction; a second substrate installation step of providing a second substrate 9 having the light-permeation material so that one surface of the second substrate 9 in the thickness direction faces the observation part 5 and the second substrate 9 is inserted in the observation part 5 in cooperation with the first substrate 3; a molded article installation step of providing a molded article 25 in a gap between the observation parts 5; and a wall part producing step of producing an opaque wall part 7 by curing the molded article 25 at the center 13 of the substrates 3, 9.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2013233696A |
source | esp@cenet |
subjects | AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING LAYERED PRODUCTS LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM PERFORMING OPERATIONS SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR SHAPING OR JOINING OF PLASTICS TRANSPORTING WORKING OF PLASTICS WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL |
title | PEEP-PREVENTING FILM AND METHOD FOR MANUFACTURING THE SAME |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-23T10%3A38%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=FUJIWARA%20SHIGERU&rft.date=2013-11-21&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2013233696A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |