METHOD FOR PRODUCTION OF RESIN COMPOSITION, RESIN COMPOSITION, AND SEMICONDUCTOR APPARATUS
PROBLEM TO BE SOLVED: To provide a method for production of a resin composition excellent in fluidity and curability at a time when sealing a semiconductor device, and to provide the resin composition and a semiconductor apparatus.SOLUTION: There is provided a method for production of a resin compos...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a method for production of a resin composition excellent in fluidity and curability at a time when sealing a semiconductor device, and to provide the resin composition and a semiconductor apparatus.SOLUTION: There is provided a method for production of a resin composition which is used for sealing a semiconductor chip 120 installed on a circuit board 110 and is also filled in an interspace between the circuit board 110 and the chip 120 when sealing. The method includes a pulverizing step of pulverizing a raw material including the powdery material of a curable resin and that of an inorganic filler in which the content of particles having the size exceeding 24 μm is 1 mass% or less, and a kneading step of kneading the raw material after pulverizing. In the kneading step, a kneading energy applied to 1 kg of the raw material after pulverizing is made to be 0.01-0.5 kWh/kg. |
---|