NEGATIVE ELECTRODE MATERIAL FOR LITHIUM ION BATTERY CONTAINING SURFACE-FLUORINATED B-TYPE TITANIUM OXIDE AND MANUFACTURING METHOD THEREOF, AND LITHIUM ION BATTERY USING THE SAME
PROBLEM TO BE SOLVED: To provide B-type titanium oxide powder which has charge and discharge characteristics and rate characteristic of B-type titanium oxide (TiO(B)) powder improved by a simple treatment and can be suitably used as a negative electrode material of a lithium ion battery.SOLUTION: B-...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | INABA MINORU TASAKA AKIMASA TAKEBAYASHI HITOSHI SAITO MORIHIRO TAKAGI MIKIHIRO HATSUSHIRO YOSHIO |
description | PROBLEM TO BE SOLVED: To provide B-type titanium oxide powder which has charge and discharge characteristics and rate characteristic of B-type titanium oxide (TiO(B)) powder improved by a simple treatment and can be suitably used as a negative electrode material of a lithium ion battery.SOLUTION: B-type titanium oxide powder is reacted at 0°C to 200°C for one minute to 10 days under fluorine-containing gas atmosphere to obtain B-type titanium oxide powder with the surface fluorinated. The fluorination treatment is preferably carried out at 0.01 atm to 2 atm. As the fluorine-containing gas, gas containing a fluorine compound selected from fluorine (F), nitrogen trifluoride (NF), methoxynitrogen trifluoride (N(CF)) and chlorine trifluoride (ClF) gases and the like is preferably used. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2013030420A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2013030420A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2013030420A3</originalsourceid><addsrcrecordid>eNqNjTEKwkAQRdNYiHqHwdpANF5gksyakWRWNrOilYislaigF_OGbsTSwuoX_73_h8lLaIXKWwJqqFRnK4IWlRxjA8Y6aFhr9i2wFShQY7OH0ooiC8sKOu8MlpSaxlvHEs0KilT3GwJlRelVu-O4ilLFZfERV-96tyWtbQVakyNrZh_i153vejpi0GFL42RwPl4eYfLNUTI1pGWdhvvtEB734ylcw_Ow3iyyeZ7l2XKRYf4X9Ably0n3</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>NEGATIVE ELECTRODE MATERIAL FOR LITHIUM ION BATTERY CONTAINING SURFACE-FLUORINATED B-TYPE TITANIUM OXIDE AND MANUFACTURING METHOD THEREOF, AND LITHIUM ION BATTERY USING THE SAME</title><source>esp@cenet</source><creator>INABA MINORU ; TASAKA AKIMASA ; TAKEBAYASHI HITOSHI ; SAITO MORIHIRO ; TAKAGI MIKIHIRO ; HATSUSHIRO YOSHIO</creator><creatorcontrib>INABA MINORU ; TASAKA AKIMASA ; TAKEBAYASHI HITOSHI ; SAITO MORIHIRO ; TAKAGI MIKIHIRO ; HATSUSHIRO YOSHIO</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide B-type titanium oxide powder which has charge and discharge characteristics and rate characteristic of B-type titanium oxide (TiO(B)) powder improved by a simple treatment and can be suitably used as a negative electrode material of a lithium ion battery.SOLUTION: B-type titanium oxide powder is reacted at 0°C to 200°C for one minute to 10 days under fluorine-containing gas atmosphere to obtain B-type titanium oxide powder with the surface fluorinated. The fluorination treatment is preferably carried out at 0.01 atm to 2 atm. As the fluorine-containing gas, gas containing a fluorine compound selected from fluorine (F), nitrogen trifluoride (NF), methoxynitrogen trifluoride (N(CF)) and chlorine trifluoride (ClF) gases and the like is preferably used.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; ELECTRICITY ; INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OFSOLID INORGANIC COMPOUNDS ; INORGANIC CHEMISTRY ; METALLURGY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2013</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20130207&DB=EPODOC&CC=JP&NR=2013030420A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25547,76298</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20130207&DB=EPODOC&CC=JP&NR=2013030420A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>INABA MINORU</creatorcontrib><creatorcontrib>TASAKA AKIMASA</creatorcontrib><creatorcontrib>TAKEBAYASHI HITOSHI</creatorcontrib><creatorcontrib>SAITO MORIHIRO</creatorcontrib><creatorcontrib>TAKAGI MIKIHIRO</creatorcontrib><creatorcontrib>HATSUSHIRO YOSHIO</creatorcontrib><title>NEGATIVE ELECTRODE MATERIAL FOR LITHIUM ION BATTERY CONTAINING SURFACE-FLUORINATED B-TYPE TITANIUM OXIDE AND MANUFACTURING METHOD THEREOF, AND LITHIUM ION BATTERY USING THE SAME</title><description>PROBLEM TO BE SOLVED: To provide B-type titanium oxide powder which has charge and discharge characteristics and rate characteristic of B-type titanium oxide (TiO(B)) powder improved by a simple treatment and can be suitably used as a negative electrode material of a lithium ion battery.SOLUTION: B-type titanium oxide powder is reacted at 0°C to 200°C for one minute to 10 days under fluorine-containing gas atmosphere to obtain B-type titanium oxide powder with the surface fluorinated. The fluorination treatment is preferably carried out at 0.01 atm to 2 atm. As the fluorine-containing gas, gas containing a fluorine compound selected from fluorine (F), nitrogen trifluoride (NF), methoxynitrogen trifluoride (N(CF)) and chlorine trifluoride (ClF) gases and the like is preferably used.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>ELECTRICITY</subject><subject>INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OFSOLID INORGANIC COMPOUNDS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2013</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjTEKwkAQRdNYiHqHwdpANF5gksyakWRWNrOilYislaigF_OGbsTSwuoX_73_h8lLaIXKWwJqqFRnK4IWlRxjA8Y6aFhr9i2wFShQY7OH0ooiC8sKOu8MlpSaxlvHEs0KilT3GwJlRelVu-O4ilLFZfERV-96tyWtbQVakyNrZh_i153vejpi0GFL42RwPl4eYfLNUTI1pGWdhvvtEB734ylcw_Ow3iyyeZ7l2XKRYf4X9Ably0n3</recordid><startdate>20130207</startdate><enddate>20130207</enddate><creator>INABA MINORU</creator><creator>TASAKA AKIMASA</creator><creator>TAKEBAYASHI HITOSHI</creator><creator>SAITO MORIHIRO</creator><creator>TAKAGI MIKIHIRO</creator><creator>HATSUSHIRO YOSHIO</creator><scope>EVB</scope></search><sort><creationdate>20130207</creationdate><title>NEGATIVE ELECTRODE MATERIAL FOR LITHIUM ION BATTERY CONTAINING SURFACE-FLUORINATED B-TYPE TITANIUM OXIDE AND MANUFACTURING METHOD THEREOF, AND LITHIUM ION BATTERY USING THE SAME</title><author>INABA MINORU ; TASAKA AKIMASA ; TAKEBAYASHI HITOSHI ; SAITO MORIHIRO ; TAKAGI MIKIHIRO ; HATSUSHIRO YOSHIO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2013030420A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2013</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>ELECTRICITY</topic><topic>INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OFSOLID INORGANIC COMPOUNDS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>INABA MINORU</creatorcontrib><creatorcontrib>TASAKA AKIMASA</creatorcontrib><creatorcontrib>TAKEBAYASHI HITOSHI</creatorcontrib><creatorcontrib>SAITO MORIHIRO</creatorcontrib><creatorcontrib>TAKAGI MIKIHIRO</creatorcontrib><creatorcontrib>HATSUSHIRO YOSHIO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>INABA MINORU</au><au>TASAKA AKIMASA</au><au>TAKEBAYASHI HITOSHI</au><au>SAITO MORIHIRO</au><au>TAKAGI MIKIHIRO</au><au>HATSUSHIRO YOSHIO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>NEGATIVE ELECTRODE MATERIAL FOR LITHIUM ION BATTERY CONTAINING SURFACE-FLUORINATED B-TYPE TITANIUM OXIDE AND MANUFACTURING METHOD THEREOF, AND LITHIUM ION BATTERY USING THE SAME</title><date>2013-02-07</date><risdate>2013</risdate><abstract>PROBLEM TO BE SOLVED: To provide B-type titanium oxide powder which has charge and discharge characteristics and rate characteristic of B-type titanium oxide (TiO(B)) powder improved by a simple treatment and can be suitably used as a negative electrode material of a lithium ion battery.SOLUTION: B-type titanium oxide powder is reacted at 0°C to 200°C for one minute to 10 days under fluorine-containing gas atmosphere to obtain B-type titanium oxide powder with the surface fluorinated. The fluorination treatment is preferably carried out at 0.01 atm to 2 atm. As the fluorine-containing gas, gas containing a fluorine compound selected from fluorine (F), nitrogen trifluoride (NF), methoxynitrogen trifluoride (N(CF)) and chlorine trifluoride (ClF) gases and the like is preferably used.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2013030420A |
source | esp@cenet |
subjects | BASIC ELECTRIC ELEMENTS CHEMISTRY COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ELECTRICITY INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OFSOLID INORGANIC COMPOUNDS INORGANIC CHEMISTRY METALLURGY PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY |
title | NEGATIVE ELECTRODE MATERIAL FOR LITHIUM ION BATTERY CONTAINING SURFACE-FLUORINATED B-TYPE TITANIUM OXIDE AND MANUFACTURING METHOD THEREOF, AND LITHIUM ION BATTERY USING THE SAME |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-16T08%3A57%3A07IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=INABA%20MINORU&rft.date=2013-02-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2013030420A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |