CONTINUOUS CASTING METHOD OF WEAR-RESISTANT STEEL
PROBLEM TO BE SOLVED: To provide a continuous casting method which can obtain a high-quality cast slab by preventing the bubble defect of a wear-resistant steel containing Ti.SOLUTION: The continuous casting method of wear-resistant steel is characterized as follows. The wear-resistant steel has a c...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a continuous casting method which can obtain a high-quality cast slab by preventing the bubble defect of a wear-resistant steel containing Ti.SOLUTION: The continuous casting method of wear-resistant steel is characterized as follows. The wear-resistant steel has a composition including 0.05-0.35 mass% of C, 0.05-1.0 mass% of Si, 0.1-2.0 mass% of Mn, 0.0003-0.0030 mass% of B, 0.1-1.0 mass% of Ti, 0.002-0.1 mass% of Al, 0.1-1.0 mass% of Cr, 0.05-1.0 mass% of Mo, 0.05-1.0 mass% of W, and a remainder consisting of Fe and inevitable impurities, the width the cast slab is 1,300-1,900 mm, a casting speed is 0.50-1.00 m/second, in addition, the flow rate Mof an Ar gas flow and the flow rate Mof an Ngas flow blown into an immersion nozzle are respectively M: 2.0-14.4 NL/second and M: 0.5-10.8 NL/second, and the continuous casting is performed in the range that the flow rate Mof the Ar gas flow and the flow rate Mof the Ngas flow satisfy 2.6≤M+1.2×M≤15.0. |
---|