METHOD FOR PRODUCING WAVELENGTH CONVERSION NANO PARTICLE AND WAVELENGTH CONVERSION NANO PARTICLE

PROBLEM TO BE SOLVED: To enable to produce wavelength conversion nano particles having a good emission intensity in an aqueous solvent.SOLUTION: (A) An aqueous solution containing a Zn ion source and NAC in a molar ratio of 1:4.8 is mixed with an aqueous solution containing a Mn ion source and NAC i...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SOFUE SUSUMU, KAWAI SHOICHI, KIN DAIKI, TAKAGI TOMOKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SOFUE SUSUMU
KAWAI SHOICHI
KIN DAIKI
TAKAGI TOMOKI
description PROBLEM TO BE SOLVED: To enable to produce wavelength conversion nano particles having a good emission intensity in an aqueous solvent.SOLUTION: (A) An aqueous solution containing a Zn ion source and NAC in a molar ratio of 1:4.8 is mixed with an aqueous solution containing a Mn ion source and NAC in a molar ratio of 1:1. (B) The former aqueous solution is mixed with the latter aqueous solution in a ratio of 10:1. Subsequently, NaOH is added to the aqueous solution to adjust the pH to 8.5, and 1.2 mmol of a Se ion source is added. In addition, (C) the aqueous solution is adjusted to pH 10.5, and then heated at 200°C under a high pressure to produce the wavelength conversion nano particles (ZnSe:Mn).
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2012219193A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2012219193A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2012219193A3</originalsourceid><addsrcrecordid>eNrjZEjwdQ3x8HdRcPMPUggI8ncJdfb0c1cIdwxz9XH1cw_xUHD29wtzDQr29PdT8HP081cIcAwK8XT2cVVw9HMhRh0PA2taYk5xKi-U5mZQcnMNcfbQTS3Ij08tLkhMTs1LLYn3CjAyMDQyMrQ0tDR2NCZKEQAWKzQz</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PRODUCING WAVELENGTH CONVERSION NANO PARTICLE AND WAVELENGTH CONVERSION NANO PARTICLE</title><source>esp@cenet</source><creator>SOFUE SUSUMU ; KAWAI SHOICHI ; KIN DAIKI ; TAKAGI TOMOKI</creator><creatorcontrib>SOFUE SUSUMU ; KAWAI SHOICHI ; KIN DAIKI ; TAKAGI TOMOKI</creatorcontrib><description>PROBLEM TO BE SOLVED: To enable to produce wavelength conversion nano particles having a good emission intensity in an aqueous solvent.SOLUTION: (A) An aqueous solution containing a Zn ion source and NAC in a molar ratio of 1:4.8 is mixed with an aqueous solution containing a Mn ion source and NAC in a molar ratio of 1:1. (B) The former aqueous solution is mixed with the latter aqueous solution in a ratio of 10:1. Subsequently, NaOH is added to the aqueous solution to adjust the pH to 8.5, and 1.2 mmol of a Se ion source is added. In addition, (C) the aqueous solution is adjusted to pH 10.5, and then heated at 200°C under a high pressure to produce the wavelength conversion nano particles (ZnSe:Mn).</description><language>eng</language><subject>ADHESIVES ; CHEMISTRY ; DYES ; MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; PAINTS ; POLISHES</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20121112&amp;DB=EPODOC&amp;CC=JP&amp;NR=2012219193A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20121112&amp;DB=EPODOC&amp;CC=JP&amp;NR=2012219193A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SOFUE SUSUMU</creatorcontrib><creatorcontrib>KAWAI SHOICHI</creatorcontrib><creatorcontrib>KIN DAIKI</creatorcontrib><creatorcontrib>TAKAGI TOMOKI</creatorcontrib><title>METHOD FOR PRODUCING WAVELENGTH CONVERSION NANO PARTICLE AND WAVELENGTH CONVERSION NANO PARTICLE</title><description>PROBLEM TO BE SOLVED: To enable to produce wavelength conversion nano particles having a good emission intensity in an aqueous solvent.SOLUTION: (A) An aqueous solution containing a Zn ion source and NAC in a molar ratio of 1:4.8 is mixed with an aqueous solution containing a Mn ion source and NAC in a molar ratio of 1:1. (B) The former aqueous solution is mixed with the latter aqueous solution in a ratio of 10:1. Subsequently, NaOH is added to the aqueous solution to adjust the pH to 8.5, and 1.2 mmol of a Se ion source is added. In addition, (C) the aqueous solution is adjusted to pH 10.5, and then heated at 200°C under a high pressure to produce the wavelength conversion nano particles (ZnSe:Mn).</description><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>DYES</subject><subject>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>PAINTS</subject><subject>POLISHES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZEjwdQ3x8HdRcPMPUggI8ncJdfb0c1cIdwxz9XH1cw_xUHD29wtzDQr29PdT8HP081cIcAwK8XT2cVVw9HMhRh0PA2taYk5xKi-U5mZQcnMNcfbQTS3Ij08tLkhMTs1LLYn3CjAyMDQyMrQ0tDR2NCZKEQAWKzQz</recordid><startdate>20121112</startdate><enddate>20121112</enddate><creator>SOFUE SUSUMU</creator><creator>KAWAI SHOICHI</creator><creator>KIN DAIKI</creator><creator>TAKAGI TOMOKI</creator><scope>EVB</scope></search><sort><creationdate>20121112</creationdate><title>METHOD FOR PRODUCING WAVELENGTH CONVERSION NANO PARTICLE AND WAVELENGTH CONVERSION NANO PARTICLE</title><author>SOFUE SUSUMU ; KAWAI SHOICHI ; KIN DAIKI ; TAKAGI TOMOKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2012219193A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2012</creationdate><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>DYES</topic><topic>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>PAINTS</topic><topic>POLISHES</topic><toplevel>online_resources</toplevel><creatorcontrib>SOFUE SUSUMU</creatorcontrib><creatorcontrib>KAWAI SHOICHI</creatorcontrib><creatorcontrib>KIN DAIKI</creatorcontrib><creatorcontrib>TAKAGI TOMOKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SOFUE SUSUMU</au><au>KAWAI SHOICHI</au><au>KIN DAIKI</au><au>TAKAGI TOMOKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PRODUCING WAVELENGTH CONVERSION NANO PARTICLE AND WAVELENGTH CONVERSION NANO PARTICLE</title><date>2012-11-12</date><risdate>2012</risdate><abstract>PROBLEM TO BE SOLVED: To enable to produce wavelength conversion nano particles having a good emission intensity in an aqueous solvent.SOLUTION: (A) An aqueous solution containing a Zn ion source and NAC in a molar ratio of 1:4.8 is mixed with an aqueous solution containing a Mn ion source and NAC in a molar ratio of 1:1. (B) The former aqueous solution is mixed with the latter aqueous solution in a ratio of 10:1. Subsequently, NaOH is added to the aqueous solution to adjust the pH to 8.5, and 1.2 mmol of a Se ion source is added. In addition, (C) the aqueous solution is adjusted to pH 10.5, and then heated at 200°C under a high pressure to produce the wavelength conversion nano particles (ZnSe:Mn).</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2012219193A
source esp@cenet
subjects ADHESIVES
CHEMISTRY
DYES
MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
PAINTS
POLISHES
title METHOD FOR PRODUCING WAVELENGTH CONVERSION NANO PARTICLE AND WAVELENGTH CONVERSION NANO PARTICLE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-20T20%3A00%3A31IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SOFUE%20SUSUMU&rft.date=2012-11-12&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2012219193A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true