METHOD OF MANUFACTURING SINTERED COMPONENT
PROBLEM TO BE SOLVED: To provide a manufacturing method for molding a favorable molding in manufacturing a minute sintered component by pressure molding a plastic raw material within a die cavity and sintering the obtained molding.SOLUTION: The method of manufacturing the sintered component includes...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a manufacturing method for molding a favorable molding in manufacturing a minute sintered component by pressure molding a plastic raw material within a die cavity and sintering the obtained molding.SOLUTION: The method of manufacturing the sintered component includes: charging the raw material prepared by adding 40-60 vol.% of a binder consisting of a thermoplastic resin and wax to a metal powder and kneading it with heat into the die cavity of a die to pressure mold it to a desired shape; pulling successively out the pressed molding from the die; removing the binder with heat; and then sintering the molding with heat. In the method, the moving speed U of a punch in pressure molding is set lower than a speed obtained by [U= P/(32μ×L)×De] with P: a punch pressing force (Pa), μ: a viscosity (Pa s), L: a length (m), and De: an equivalent pipe diameter (m). |
---|