NON-ALKALI GLASS, ITS PRODUCTION METHOD, AND GLASS SUBSTRATE FOR FORMING TFT (THIN FILM TRANSISTOR) OF LIQUID CRYSTAL DISPLAY
PROBLEM TO BE SOLVED: To provide a non-alkali glass which has characteristics such as chemical durability, low thermal expansion property, high strain point, low specific gravity and high Young's modulus, has less defects such as foams and is excellent in production stability.SOLUTION: The non-...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | HACHITANI YOICHI |
description | PROBLEM TO BE SOLVED: To provide a non-alkali glass which has characteristics such as chemical durability, low thermal expansion property, high strain point, low specific gravity and high Young's modulus, has less defects such as foams and is excellent in production stability.SOLUTION: The non-alkali glass has: an average thermal expansion coefficient at 30-300°C in the range of (30-35)×10/°C; strain point of at least 670°C; Young's modulus of at least 70 GPa; specific gravity of less than 2.4; liquid phase temperature of less than 1,200°C; temperature showing the viscosity of 10Pa s of less than 1.600°C; and less than 1 mg/cmof the mass decrease after the immersion in an aqueous solution of nitric acid at 50°C having the concentration of 1 mol/L for 50 hr. The glass contains, by mol, 65.0-70.0% of SiO, 9.5-12.5% of AlO, 8.5-11.5% of BO(provided that SiO+AlO+BOis 87.5-90.0 mol%, and BO/(SiO+AlO) is 0.12-0.14), 2.5 to less than 4.0% of MgO, 5.0-10.0% of CaO, 0.1-2.5% of SrO (provided that MgO+CaO+SrO is 10.0-12.5 mol%), and does not substantially contain BaO, ZnO and PbO. |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2012176887A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2012176887A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2012176887A3</originalsourceid><addsrcrecordid>eNqNyrEOgjAQgGEWB6O-w8VJE0gEE3WtlMJpabF3DEyEmDoZJcHVd1ejD-Dw51--cfA01kRCH4VGyLUgCgGZoHJW1imjNVBmXFgZgjDyK4DqPbETnIGy7lOJJgdWDAsu0IBCXcIbGEJi65ZgFWg81SghdQ2x0CCRKi2aaTC6dNfBz36fBHOVcVpEvr-3fui7s7_5R3uoklWcxNvNbrcV67_QCwUJO6c</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>NON-ALKALI GLASS, ITS PRODUCTION METHOD, AND GLASS SUBSTRATE FOR FORMING TFT (THIN FILM TRANSISTOR) OF LIQUID CRYSTAL DISPLAY</title><source>esp@cenet</source><creator>HACHITANI YOICHI</creator><creatorcontrib>HACHITANI YOICHI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a non-alkali glass which has characteristics such as chemical durability, low thermal expansion property, high strain point, low specific gravity and high Young's modulus, has less defects such as foams and is excellent in production stability.SOLUTION: The non-alkali glass has: an average thermal expansion coefficient at 30-300°C in the range of (30-35)×10/°C; strain point of at least 670°C; Young's modulus of at least 70 GPa; specific gravity of less than 2.4; liquid phase temperature of less than 1,200°C; temperature showing the viscosity of 10Pa s of less than 1.600°C; and less than 1 mg/cmof the mass decrease after the immersion in an aqueous solution of nitric acid at 50°C having the concentration of 1 mol/L for 50 hr. The glass contains, by mol, 65.0-70.0% of SiO, 9.5-12.5% of AlO, 8.5-11.5% of BO(provided that SiO+AlO+BOis 87.5-90.0 mol%, and BO/(SiO+AlO) is 0.12-0.14), 2.5 to less than 4.0% of MgO, 5.0-10.0% of CaO, 0.1-2.5% of SrO (provided that MgO+CaO+SrO is 10.0-12.5 mol%), and does not substantially contain BaO, ZnO and PbO.</description><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; DEVICES OR ARRANGEMENTS, THE OPTICAL OPERATION OF WHICH ISMODIFIED BY CHANGING THE OPTICAL PROPERTIES OF THE MEDIUM OF THEDEVICES OR ARRANGEMENTS FOR THE CONTROL OF THE INTENSITY,COLOUR, PHASE, POLARISATION OR DIRECTION OF LIGHT, e.g.SWITCHING, GATING, MODULATING OR DEMODULATING ; FREQUENCY-CHANGING ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; METALLURGY ; MINERAL OR SLAG WOOL ; NON-LINEAR OPTICS ; OPTICAL ANALOGUE/DIGITAL CONVERTERS ; OPTICAL LOGIC ELEMENTS ; OPTICS ; PHYSICS ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS ; TECHNIQUES OR PROCEDURES FOR THE OPERATION THEREOF</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20120913&DB=EPODOC&CC=JP&NR=2012176887A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20120913&DB=EPODOC&CC=JP&NR=2012176887A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HACHITANI YOICHI</creatorcontrib><title>NON-ALKALI GLASS, ITS PRODUCTION METHOD, AND GLASS SUBSTRATE FOR FORMING TFT (THIN FILM TRANSISTOR) OF LIQUID CRYSTAL DISPLAY</title><description>PROBLEM TO BE SOLVED: To provide a non-alkali glass which has characteristics such as chemical durability, low thermal expansion property, high strain point, low specific gravity and high Young's modulus, has less defects such as foams and is excellent in production stability.SOLUTION: The non-alkali glass has: an average thermal expansion coefficient at 30-300°C in the range of (30-35)×10/°C; strain point of at least 670°C; Young's modulus of at least 70 GPa; specific gravity of less than 2.4; liquid phase temperature of less than 1,200°C; temperature showing the viscosity of 10Pa s of less than 1.600°C; and less than 1 mg/cmof the mass decrease after the immersion in an aqueous solution of nitric acid at 50°C having the concentration of 1 mol/L for 50 hr. The glass contains, by mol, 65.0-70.0% of SiO, 9.5-12.5% of AlO, 8.5-11.5% of BO(provided that SiO+AlO+BOis 87.5-90.0 mol%, and BO/(SiO+AlO) is 0.12-0.14), 2.5 to less than 4.0% of MgO, 5.0-10.0% of CaO, 0.1-2.5% of SrO (provided that MgO+CaO+SrO is 10.0-12.5 mol%), and does not substantially contain BaO, ZnO and PbO.</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>DEVICES OR ARRANGEMENTS, THE OPTICAL OPERATION OF WHICH ISMODIFIED BY CHANGING THE OPTICAL PROPERTIES OF THE MEDIUM OF THEDEVICES OR ARRANGEMENTS FOR THE CONTROL OF THE INTENSITY,COLOUR, PHASE, POLARISATION OR DIRECTION OF LIGHT, e.g.SWITCHING, GATING, MODULATING OR DEMODULATING</subject><subject>FREQUENCY-CHANGING</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>NON-LINEAR OPTICS</subject><subject>OPTICAL ANALOGUE/DIGITAL CONVERTERS</subject><subject>OPTICAL LOGIC ELEMENTS</subject><subject>OPTICS</subject><subject>PHYSICS</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><subject>TECHNIQUES OR PROCEDURES FOR THE OPERATION THEREOF</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEOgjAQgGEWB6O-w8VJE0gEE3WtlMJpabF3DEyEmDoZJcHVd1ejD-Dw51--cfA01kRCH4VGyLUgCgGZoHJW1imjNVBmXFgZgjDyK4DqPbETnIGy7lOJJgdWDAsu0IBCXcIbGEJi65ZgFWg81SghdQ2x0CCRKi2aaTC6dNfBz36fBHOVcVpEvr-3fui7s7_5R3uoklWcxNvNbrcV67_QCwUJO6c</recordid><startdate>20120913</startdate><enddate>20120913</enddate><creator>HACHITANI YOICHI</creator><scope>EVB</scope></search><sort><creationdate>20120913</creationdate><title>NON-ALKALI GLASS, ITS PRODUCTION METHOD, AND GLASS SUBSTRATE FOR FORMING TFT (THIN FILM TRANSISTOR) OF LIQUID CRYSTAL DISPLAY</title><author>HACHITANI YOICHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2012176887A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2012</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>DEVICES OR ARRANGEMENTS, THE OPTICAL OPERATION OF WHICH ISMODIFIED BY CHANGING THE OPTICAL PROPERTIES OF THE MEDIUM OF THEDEVICES OR ARRANGEMENTS FOR THE CONTROL OF THE INTENSITY,COLOUR, PHASE, POLARISATION OR DIRECTION OF LIGHT, e.g.SWITCHING, GATING, MODULATING OR DEMODULATING</topic><topic>FREQUENCY-CHANGING</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>NON-LINEAR OPTICS</topic><topic>OPTICAL ANALOGUE/DIGITAL CONVERTERS</topic><topic>OPTICAL LOGIC ELEMENTS</topic><topic>OPTICS</topic><topic>PHYSICS</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><topic>TECHNIQUES OR PROCEDURES FOR THE OPERATION THEREOF</topic><toplevel>online_resources</toplevel><creatorcontrib>HACHITANI YOICHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HACHITANI YOICHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>NON-ALKALI GLASS, ITS PRODUCTION METHOD, AND GLASS SUBSTRATE FOR FORMING TFT (THIN FILM TRANSISTOR) OF LIQUID CRYSTAL DISPLAY</title><date>2012-09-13</date><risdate>2012</risdate><abstract>PROBLEM TO BE SOLVED: To provide a non-alkali glass which has characteristics such as chemical durability, low thermal expansion property, high strain point, low specific gravity and high Young's modulus, has less defects such as foams and is excellent in production stability.SOLUTION: The non-alkali glass has: an average thermal expansion coefficient at 30-300°C in the range of (30-35)×10/°C; strain point of at least 670°C; Young's modulus of at least 70 GPa; specific gravity of less than 2.4; liquid phase temperature of less than 1,200°C; temperature showing the viscosity of 10Pa s of less than 1.600°C; and less than 1 mg/cmof the mass decrease after the immersion in an aqueous solution of nitric acid at 50°C having the concentration of 1 mol/L for 50 hr. The glass contains, by mol, 65.0-70.0% of SiO, 9.5-12.5% of AlO, 8.5-11.5% of BO(provided that SiO+AlO+BOis 87.5-90.0 mol%, and BO/(SiO+AlO) is 0.12-0.14), 2.5 to less than 4.0% of MgO, 5.0-10.0% of CaO, 0.1-2.5% of SrO (provided that MgO+CaO+SrO is 10.0-12.5 mol%), and does not substantially contain BaO, ZnO and PbO.</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2012176887A |
source | esp@cenet |
subjects | CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS CHEMISTRY DEVICES OR ARRANGEMENTS, THE OPTICAL OPERATION OF WHICH ISMODIFIED BY CHANGING THE OPTICAL PROPERTIES OF THE MEDIUM OF THEDEVICES OR ARRANGEMENTS FOR THE CONTROL OF THE INTENSITY,COLOUR, PHASE, POLARISATION OR DIRECTION OF LIGHT, e.g.SWITCHING, GATING, MODULATING OR DEMODULATING FREQUENCY-CHANGING GLASS JOINING GLASS TO GLASS OR OTHER MATERIALS METALLURGY MINERAL OR SLAG WOOL NON-LINEAR OPTICS OPTICAL ANALOGUE/DIGITAL CONVERTERS OPTICAL LOGIC ELEMENTS OPTICS PHYSICS SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS SURFACE TREATMENT OF GLASS TECHNIQUES OR PROCEDURES FOR THE OPERATION THEREOF |
title | NON-ALKALI GLASS, ITS PRODUCTION METHOD, AND GLASS SUBSTRATE FOR FORMING TFT (THIN FILM TRANSISTOR) OF LIQUID CRYSTAL DISPLAY |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T12%3A56%3A19IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HACHITANI%20YOICHI&rft.date=2012-09-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2012176887A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |