METHOD FOR MANUFACTURING OPTICAL FILM

PROBLEM TO BE SOLVED: To provide a method for manufacturing an optical film comprising an acrylic resin, in which the optical film achieves the reduction of sticking of foreign matters or occurrence of flaws and improves optical characteristics such as retardation unevenness although the optical fil...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHIROSHIMA SATOHIRO, UKAMURA TADAYOSHI, NIWA HIROKAZU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SHIROSHIMA SATOHIRO
UKAMURA TADAYOSHI
NIWA HIROKAZU
description PROBLEM TO BE SOLVED: To provide a method for manufacturing an optical film comprising an acrylic resin, in which the optical film achieves the reduction of sticking of foreign matters or occurrence of flaws and improves optical characteristics such as retardation unevenness although the optical film includes an easily-adhesive layer and is subjected to trimming processing.SOLUTION: A method for manufacturing an optical film comprises: a step of melting a thermoplastic resin including an acrylic polymer and film-forming to form the belt-shaped original film; a step of longitudinally stretching the formed original film; a step of laterally stretching the longitudinally stretched original film to form an optical film; and a step of winding the optical film, and these steps are continuously executed. The method further comprises a step of applying an easily-adhesive composition on a surface of the original film between the longitudinal stretching step and the lateral stretching step. In the lateral stretching step, the applied film of the easily-adhesive composition formed on the surface of the film is dried by the heat applied to the original film to form an easily-adhesive layer. The method further comprises a step of trimming the optical film between the lateral stretching step and the winding step.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2012118479A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2012118479A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2012118479A3</originalsourceid><addsrcrecordid>eNrjZFD1dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNX8A8I8XR29FFw8_Tx5WFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgaGRoaGFibmlo7GRCkCAOMXI7Y</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING OPTICAL FILM</title><source>esp@cenet</source><creator>SHIROSHIMA SATOHIRO ; UKAMURA TADAYOSHI ; NIWA HIROKAZU</creator><creatorcontrib>SHIROSHIMA SATOHIRO ; UKAMURA TADAYOSHI ; NIWA HIROKAZU</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing an optical film comprising an acrylic resin, in which the optical film achieves the reduction of sticking of foreign matters or occurrence of flaws and improves optical characteristics such as retardation unevenness although the optical film includes an easily-adhesive layer and is subjected to trimming processing.SOLUTION: A method for manufacturing an optical film comprises: a step of melting a thermoplastic resin including an acrylic polymer and film-forming to form the belt-shaped original film; a step of longitudinally stretching the formed original film; a step of laterally stretching the longitudinally stretched original film to form an optical film; and a step of winding the optical film, and these steps are continuously executed. The method further comprises a step of applying an easily-adhesive composition on a surface of the original film between the longitudinal stretching step and the lateral stretching step. In the lateral stretching step, the applied film of the easily-adhesive composition formed on the surface of the film is dried by the heat applied to the original film to form an easily-adhesive layer. The method further comprises a step of trimming the optical film between the lateral stretching step and the winding step.</description><language>eng</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; GENERAL PROCESSES OF COMPOUNDING ; INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES ; INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS ; METALLURGY ; OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS ; OPTICS ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; PHYSICS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL ; WORKING-UP</subject><creationdate>2012</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120621&amp;DB=EPODOC&amp;CC=JP&amp;NR=2012118479A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20120621&amp;DB=EPODOC&amp;CC=JP&amp;NR=2012118479A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SHIROSHIMA SATOHIRO</creatorcontrib><creatorcontrib>UKAMURA TADAYOSHI</creatorcontrib><creatorcontrib>NIWA HIROKAZU</creatorcontrib><title>METHOD FOR MANUFACTURING OPTICAL FILM</title><description>PROBLEM TO BE SOLVED: To provide a method for manufacturing an optical film comprising an acrylic resin, in which the optical film achieves the reduction of sticking of foreign matters or occurrence of flaws and improves optical characteristics such as retardation unevenness although the optical film includes an easily-adhesive layer and is subjected to trimming processing.SOLUTION: A method for manufacturing an optical film comprises: a step of melting a thermoplastic resin including an acrylic polymer and film-forming to form the belt-shaped original film; a step of longitudinally stretching the formed original film; a step of laterally stretching the longitudinally stretched original film to form an optical film; and a step of winding the optical film, and these steps are continuously executed. The method further comprises a step of applying an easily-adhesive composition on a surface of the original film between the longitudinal stretching step and the lateral stretching step. In the lateral stretching step, the applied film of the easily-adhesive composition formed on the surface of the film is dried by the heat applied to the original film to form an easily-adhesive layer. The method further comprises a step of trimming the optical film between the lateral stretching step and the winding step.</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES</subject><subject>INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS</subject><subject>METALLURGY</subject><subject>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</subject><subject>OPTICS</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2012</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFD1dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNX8A8I8XR29FFw8_Tx5WFgTUvMKU7lhdLcDEpuriHOHrqpBfnxqcUFicmpeakl8V4BRgaGRoaGFibmlo7GRCkCAOMXI7Y</recordid><startdate>20120621</startdate><enddate>20120621</enddate><creator>SHIROSHIMA SATOHIRO</creator><creator>UKAMURA TADAYOSHI</creator><creator>NIWA HIROKAZU</creator><scope>EVB</scope></search><sort><creationdate>20120621</creationdate><title>METHOD FOR MANUFACTURING OPTICAL FILM</title><author>SHIROSHIMA SATOHIRO ; UKAMURA TADAYOSHI ; NIWA HIROKAZU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2012118479A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2012</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES</topic><topic>INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS</topic><topic>METALLURGY</topic><topic>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</topic><topic>OPTICS</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>SHIROSHIMA SATOHIRO</creatorcontrib><creatorcontrib>UKAMURA TADAYOSHI</creatorcontrib><creatorcontrib>NIWA HIROKAZU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SHIROSHIMA SATOHIRO</au><au>UKAMURA TADAYOSHI</au><au>NIWA HIROKAZU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING OPTICAL FILM</title><date>2012-06-21</date><risdate>2012</risdate><abstract>PROBLEM TO BE SOLVED: To provide a method for manufacturing an optical film comprising an acrylic resin, in which the optical film achieves the reduction of sticking of foreign matters or occurrence of flaws and improves optical characteristics such as retardation unevenness although the optical film includes an easily-adhesive layer and is subjected to trimming processing.SOLUTION: A method for manufacturing an optical film comprises: a step of melting a thermoplastic resin including an acrylic polymer and film-forming to form the belt-shaped original film; a step of longitudinally stretching the formed original film; a step of laterally stretching the longitudinally stretched original film to form an optical film; and a step of winding the optical film, and these steps are continuously executed. The method further comprises a step of applying an easily-adhesive composition on a surface of the original film between the longitudinal stretching step and the lateral stretching step. In the lateral stretching step, the applied film of the easily-adhesive composition formed on the surface of the film is dried by the heat applied to the original film to form an easily-adhesive layer. The method further comprises a step of trimming the optical film between the lateral stretching step and the winding step.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2012118479A
source esp@cenet
subjects AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G
AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
GENERAL PROCESSES OF COMPOUNDING
INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES
INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS
METALLURGY
OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
OPTICS
ORGANIC MACROMOLECULAR COMPOUNDS
PERFORMING OPERATIONS
PHYSICS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
THEIR PREPARATION OR CHEMICAL WORKING-UP
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
WORKING-UP
title METHOD FOR MANUFACTURING OPTICAL FILM
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-04T23%3A08%3A08IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SHIROSHIMA%20SATOHIRO&rft.date=2012-06-21&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2012118479A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true