FOAM BLOW MOLDING METHOD
PROBLEM TO BE SOLVED: To provide a method of manufacturing a blow molded plastic material with a high expansion ratio.SOLUTION: Plastic contains a pyrogenic foaming agent. After clamping molds, air in a cavity 4 between a parison 1 and molds 2, 3 is sucked for depressurization as a first step, and a...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a method of manufacturing a blow molded plastic material with a high expansion ratio.SOLUTION: Plastic contains a pyrogenic foaming agent. After clamping molds, air in a cavity 4 between a parison 1 and molds 2, 3 is sucked for depressurization as a first step, and at the same time, air is sucked from a blow pin 7 that communicates with an atmosphere into the parison 1, and the parison 1 is expanded to be brought into tight contact with inner surfaces of the molds 2, 3. While continuing depressurization of the inside of the cavity 4, the air in the parison 1 is sucked from the blow pin 7 to depressurize the inside of the parison 1 as a second step. While maintaining depressurized states in the cavity 4 and parison 1, the parison 1 is cooled. The depressurized states are released and the molds are opened to take out a product. |
---|