MANUFACTURING METHOD FOR POLYMER, POLYMER, THERMOPLASTIC COMPOSITION AND MOLDED BODY

PROBLEM TO BE SOLVED: To provide a polymer that is readily radically polymerized, exhibits heat resistance, is inhibited from thermal decomposition when molded, is formed into a molded body excellent in external appearances and mechanical properties, and is suitable for applications for optical mate...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: NODONO MITSUFUMI, ONUMA TAEKO, NODA TETSUYA
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a polymer that is readily radically polymerized, exhibits heat resistance, is inhibited from thermal decomposition when molded, is formed into a molded body excellent in external appearances and mechanical properties, and is suitable for applications for optical materials. SOLUTION: The manufacturing method comprises radically polymerizing a monomer component comprising a monomer (a) represented by formula (1) in the presence of a chain transfer agent in an organic solvent. The polymer is obtained by the method. In the formula, R1is hydrogen or a methyl group; and R2is a cyano group bonded to any one of an ortho-position, a meta-position and a para-position of the benzene ring. COPYRIGHT: (C)2011,JPO&INPIT