FINE PARTICLE SYNTHESIS METHOD AND ELECTRONIC-COMPONENT MANUFACTURING METHOD

PROBLEM TO BE SOLVED: To provide a synthesis method of fine particles, reducing corrosion of a reaction container and the like, preventing an impurity due to the corrosion from being mixed into a product, and broadening choices of materials of the reaction container and the like. SOLUTION: The synth...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KO KINTO, IMURA TOMOYA, NAKAHATA ISAO, MASUZAWA KIYOYUKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KO KINTO
IMURA TOMOYA
NAKAHATA ISAO
MASUZAWA KIYOYUKI
description PROBLEM TO BE SOLVED: To provide a synthesis method of fine particles, reducing corrosion of a reaction container and the like, preventing an impurity due to the corrosion from being mixed into a product, and broadening choices of materials of the reaction container and the like. SOLUTION: The synthesis method of fine particles includes: creating a subcritical or supercritical reaction environment by at least one of heat and pressure by using a mixed medium comprising water and a solvent which makes the mixed medium into a supercritical state at a lower temperature and a lower pressure than those in the case of water alone; and leaving source materials under the created subcritical or supercritical reaction environment as a reaction field for a predetermined time to produce fine particles. By this method, critical conditions to create a subcritical or supercritical state can be alleviated in comparison with the case of water alone. COPYRIGHT: (C)2010,JPO&INPIT
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2010105904A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2010105904A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2010105904A3</originalsourceid><addsrcrecordid>eNrjZPBx8_RzVQhwDArxdPZxVQiO9AvxcA32DFbwdQ3x8HdRcPRzUXD1cXUOCfL383TWdfb3DfD3c_ULUfB19At1c3QOCQ3y9HOHquZhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhkBoamlg4mhMlCIAOKMupA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>FINE PARTICLE SYNTHESIS METHOD AND ELECTRONIC-COMPONENT MANUFACTURING METHOD</title><source>esp@cenet</source><creator>KO KINTO ; IMURA TOMOYA ; NAKAHATA ISAO ; MASUZAWA KIYOYUKI</creator><creatorcontrib>KO KINTO ; IMURA TOMOYA ; NAKAHATA ISAO ; MASUZAWA KIYOYUKI</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a synthesis method of fine particles, reducing corrosion of a reaction container and the like, preventing an impurity due to the corrosion from being mixed into a product, and broadening choices of materials of the reaction container and the like. SOLUTION: The synthesis method of fine particles includes: creating a subcritical or supercritical reaction environment by at least one of heat and pressure by using a mixed medium comprising water and a solvent which makes the mixed medium into a supercritical state at a lower temperature and a lower pressure than those in the case of water alone; and leaving source materials under the created subcritical or supercritical reaction environment as a reaction field for a predetermined time to produce fine particles. By this method, critical conditions to create a subcritical or supercritical state can be alleviated in comparison with the case of water alone. COPYRIGHT: (C)2010,JPO&amp;INPIT</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; CAPACITORS ; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE ; CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; ELECTRICITY ; INORGANIC CHEMISTRY ; METALLURGY</subject><creationdate>2010</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20100513&amp;DB=EPODOC&amp;CC=JP&amp;NR=2010105904A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20100513&amp;DB=EPODOC&amp;CC=JP&amp;NR=2010105904A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KO KINTO</creatorcontrib><creatorcontrib>IMURA TOMOYA</creatorcontrib><creatorcontrib>NAKAHATA ISAO</creatorcontrib><creatorcontrib>MASUZAWA KIYOYUKI</creatorcontrib><title>FINE PARTICLE SYNTHESIS METHOD AND ELECTRONIC-COMPONENT MANUFACTURING METHOD</title><description>PROBLEM TO BE SOLVED: To provide a synthesis method of fine particles, reducing corrosion of a reaction container and the like, preventing an impurity due to the corrosion from being mixed into a product, and broadening choices of materials of the reaction container and the like. SOLUTION: The synthesis method of fine particles includes: creating a subcritical or supercritical reaction environment by at least one of heat and pressure by using a mixed medium comprising water and a solvent which makes the mixed medium into a supercritical state at a lower temperature and a lower pressure than those in the case of water alone; and leaving source materials under the created subcritical or supercritical reaction environment as a reaction field for a predetermined time to produce fine particles. By this method, critical conditions to create a subcritical or supercritical state can be alleviated in comparison with the case of water alone. COPYRIGHT: (C)2010,JPO&amp;INPIT</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CAPACITORS</subject><subject>CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>ELECTRICITY</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2010</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPBx8_RzVQhwDArxdPZxVQiO9AvxcA32DFbwdQ3x8HdRcPRzUXD1cXUOCfL383TWdfb3DfD3c_ULUfB19At1c3QOCQ3y9HOHquZhYE1LzClO5YXS3AxKbq4hzh66qQX58anFBYnJqXmpJfFeAUYGhkBoamlg4mhMlCIAOKMupA</recordid><startdate>20100513</startdate><enddate>20100513</enddate><creator>KO KINTO</creator><creator>IMURA TOMOYA</creator><creator>NAKAHATA ISAO</creator><creator>MASUZAWA KIYOYUKI</creator><scope>EVB</scope></search><sort><creationdate>20100513</creationdate><title>FINE PARTICLE SYNTHESIS METHOD AND ELECTRONIC-COMPONENT MANUFACTURING METHOD</title><author>KO KINTO ; IMURA TOMOYA ; NAKAHATA ISAO ; MASUZAWA KIYOYUKI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2010105904A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2010</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CAPACITORS</topic><topic>CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>ELECTRICITY</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><toplevel>online_resources</toplevel><creatorcontrib>KO KINTO</creatorcontrib><creatorcontrib>IMURA TOMOYA</creatorcontrib><creatorcontrib>NAKAHATA ISAO</creatorcontrib><creatorcontrib>MASUZAWA KIYOYUKI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KO KINTO</au><au>IMURA TOMOYA</au><au>NAKAHATA ISAO</au><au>MASUZAWA KIYOYUKI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>FINE PARTICLE SYNTHESIS METHOD AND ELECTRONIC-COMPONENT MANUFACTURING METHOD</title><date>2010-05-13</date><risdate>2010</risdate><abstract>PROBLEM TO BE SOLVED: To provide a synthesis method of fine particles, reducing corrosion of a reaction container and the like, preventing an impurity due to the corrosion from being mixed into a product, and broadening choices of materials of the reaction container and the like. SOLUTION: The synthesis method of fine particles includes: creating a subcritical or supercritical reaction environment by at least one of heat and pressure by using a mixed medium comprising water and a solvent which makes the mixed medium into a supercritical state at a lower temperature and a lower pressure than those in the case of water alone; and leaving source materials under the created subcritical or supercritical reaction environment as a reaction field for a predetermined time to produce fine particles. By this method, critical conditions to create a subcritical or supercritical state can be alleviated in comparison with the case of water alone. COPYRIGHT: (C)2010,JPO&amp;INPIT</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2010105904A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CAPACITORS
CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES ORLIGHT-SENSITIVE DEVICES, OF THE ELECTROLYTIC TYPE
CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
ELECTRICITY
INORGANIC CHEMISTRY
METALLURGY
title FINE PARTICLE SYNTHESIS METHOD AND ELECTRONIC-COMPONENT MANUFACTURING METHOD
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-01T19%3A51%3A51IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KO%20KINTO&rft.date=2010-05-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2010105904A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true