ALLOY AND TUBE FOR NUCLEAR FUEL ASSEMBLY
PROBLEM TO BE SOLVED: To provide a method for making tubes designed for a nuclear fuel pencil case or guide tube. SOLUTION: The tube is made from a bar of a zirconium based alloy, and contains 0.03 to 0.25 wt.% total of iron and chromium or vanadium, 0.8 to 1.3 wt.% niobium, ≤2,000 ppm tin, 500 to 2...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a method for making tubes designed for a nuclear fuel pencil case or guide tube. SOLUTION: The tube is made from a bar of a zirconium based alloy, and contains 0.03 to 0.25 wt.% total of iron and chromium or vanadium, 0.8 to 1.3 wt.% niobium, ≤2,000 ppm tin, 500 to 2,000 ppm oxygen, ≤100 ppm carbon, 5 to 35 ppm sulphur and ≤50 ppm silicon. The bar is soaked in water after being heated at 1,000°C to 1,200°C. The blank is extruded after being heated at 600 to 800°C, and is cold-rolled in at least four passes, to obtain a tube, and is performed with intermediate heat treatment at 560 to 620°C, and is performed with a final heat treatment at 560 to 620°C in inert atmosphere or under vacuum. COPYRIGHT: (C)2010,JPO&INPIT |
---|