RESISTANCE ALLOY

PROBLEM TO BE SOLVED: To provide a resistance alloy having high volume resistivity and excellent temperature properties, and further having excellent hot workability. SOLUTION: The resistance alloy has a chemical composition comprising, by mass, 27.5 to 35% Mn, 8 to 10% Al, 5 to 7% Cr and 1.0 to 1.2...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ISHIO MASAAKI, ISHIDA KIYOHITO, SUDO YUJI, SHIOMI KAZUHIRO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a resistance alloy having high volume resistivity and excellent temperature properties, and further having excellent hot workability. SOLUTION: The resistance alloy has a chemical composition comprising, by mass, 27.5 to 35% Mn, 8 to 10% Al, 5 to 7% Cr and 1.0 to 1.2% C, and the balance Fe with inevitable impurities. The fundamental components can comprise one or more elements selected from ≤1.5% B, ≤1.5% N, one or two selected from an Mg group (Mg and Si) by ≤5.0% in total, one or two selected from a Ti group (Ti and Mo) by ≤5.0% in total, one or two selected from a Co group (Co and Ni) by ≤5.0% in total and ≤5.0% W. COPYRIGHT: (C)2010,JPO&INPIT