SURFACE-MODIFIED INORGANIC OXIDE POWDER AND TONER COMPOSITION FOR ELECTROPHOTOGRAPHY

PROBLEM TO BE SOLVED: To provide a surface-modified inorganic oxide powder subjected to a surface treatment with a silicone oil, having a high fixation rate of the silicone oil and high hydrophobicity. SOLUTION: The inorganic oxide powder subjected to a surface treatment with a reactive modified sil...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: INOUE AKIRA, TASHIRO HIDEAKI, KANAE MASAATSU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PROBLEM TO BE SOLVED: To provide a surface-modified inorganic oxide powder subjected to a surface treatment with a silicone oil, having a high fixation rate of the silicone oil and high hydrophobicity. SOLUTION: The inorganic oxide powder subjected to a surface treatment with a reactive modified silicone oil has a carbon fixation rate of not less than 90% and a hydrophobicity rate of not less than 95%. The inorganic oxide powder includes, preferably fumed silica. The surface-modified inorganic oxide powder is obtained by adding a reactive modified silicone oil to an inorganic oxide powder and subjecting the powder to a primary treatment at 150 to 280°C, followed by a secondary treatment over 280°C. By carrying out the surface treatment using the reactive modified silicone oil in a two-step treatment under predetermined temperature conditions, the obtained surface-modified inorganic oxide powder has a high fixation rate and high hydrophobicity. COPYRIGHT: (C)2010,JPO&INPIT