METHOD FOR MANUFACTURING ANTIREFLECTION FILM, ANTIREFLECTION FILM, POLARIZING PLATE, AND IMAGE DISPLAY DEVICE
PROBLEM TO BE SOLVED: To provide an antireflection film which is excellent in chemical resistance, adhesiveness and scuff resistance after moisture and heat treatment such as in a high temperature and high humidity environment, and is inexpensive since properties of a thin film can be improved by fo...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | OKANO MASARU |
description | PROBLEM TO BE SOLVED: To provide an antireflection film which is excellent in chemical resistance, adhesiveness and scuff resistance after moisture and heat treatment such as in a high temperature and high humidity environment, and is inexpensive since properties of a thin film can be improved by forming an antireflection layer made of one low-refractive index layer. SOLUTION: The method for manufacturing antireflection film includes: a process of providing a hard coat layer directly or via other layer on a film base; and further laminating a low-refractive index layer on the hard coat layer, wherein the hard coat layer contains at least one kind of compound having an HLB value of 3 to 18 and, further, the surface of the hard coat layer is surface-treated and, thereafter, the low-refractive index layer containing at least one kind of hollow silica based particles each of which has an outer shell layer and a porous and hollow interior is laminated on the surface of the hard coat layer. COPYRIGHT: (C)2009,JPO&INPIT |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2009210876A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2009210876A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2009210876A3</originalsourceid><addsrcrecordid>eNrjZMj1dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXcPQL8QxydfNxdQ7x9PdTcPP08dXBLhjg7-MY5BkF0hTg4xjiClLmouDp6-juquDiGQwUi1RwcQ3zdHblYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgaWRoYGFuZmjsZEKQIAkFE3PQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR MANUFACTURING ANTIREFLECTION FILM, ANTIREFLECTION FILM, POLARIZING PLATE, AND IMAGE DISPLAY DEVICE</title><source>esp@cenet</source><creator>OKANO MASARU</creator><creatorcontrib>OKANO MASARU</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide an antireflection film which is excellent in chemical resistance, adhesiveness and scuff resistance after moisture and heat treatment such as in a high temperature and high humidity environment, and is inexpensive since properties of a thin film can be improved by forming an antireflection layer made of one low-refractive index layer. SOLUTION: The method for manufacturing antireflection film includes: a process of providing a hard coat layer directly or via other layer on a film base; and further laminating a low-refractive index layer on the hard coat layer, wherein the hard coat layer contains at least one kind of compound having an HLB value of 3 to 18 and, further, the surface of the hard coat layer is surface-treated and, thereafter, the low-refractive index layer containing at least one kind of hollow silica based particles each of which has an outer shell layer and a porous and hollow interior is laminated on the surface of the hard coat layer. COPYRIGHT: (C)2009,JPO&INPIT</description><language>eng</language><subject>LAYERED PRODUCTS ; LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM ; OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS ; OPTICS ; PERFORMING OPERATIONS ; PHYSICS ; TRANSPORTING</subject><creationdate>2009</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20090917&DB=EPODOC&CC=JP&NR=2009210876A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25562,76317</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20090917&DB=EPODOC&CC=JP&NR=2009210876A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>OKANO MASARU</creatorcontrib><title>METHOD FOR MANUFACTURING ANTIREFLECTION FILM, ANTIREFLECTION FILM, POLARIZING PLATE, AND IMAGE DISPLAY DEVICE</title><description>PROBLEM TO BE SOLVED: To provide an antireflection film which is excellent in chemical resistance, adhesiveness and scuff resistance after moisture and heat treatment such as in a high temperature and high humidity environment, and is inexpensive since properties of a thin film can be improved by forming an antireflection layer made of one low-refractive index layer. SOLUTION: The method for manufacturing antireflection film includes: a process of providing a hard coat layer directly or via other layer on a film base; and further laminating a low-refractive index layer on the hard coat layer, wherein the hard coat layer contains at least one kind of compound having an HLB value of 3 to 18 and, further, the surface of the hard coat layer is surface-treated and, thereafter, the low-refractive index layer containing at least one kind of hollow silica based particles each of which has an outer shell layer and a porous and hollow interior is laminated on the surface of the hard coat layer. COPYRIGHT: (C)2009,JPO&INPIT</description><subject>LAYERED PRODUCTS</subject><subject>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</subject><subject>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</subject><subject>OPTICS</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICS</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2009</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZMj1dQ3x8HdRcPMPUvB19At1c3QOCQ3y9HNXcPQL8QxydfNxdQ7x9PdTcPP08dXBLhjg7-MY5BkF0hTg4xjiClLmouDp6-juquDiGQwUi1RwcQ3zdHblYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgaWRoYGFuZmjsZEKQIAkFE3PQ</recordid><startdate>20090917</startdate><enddate>20090917</enddate><creator>OKANO MASARU</creator><scope>EVB</scope></search><sort><creationdate>20090917</creationdate><title>METHOD FOR MANUFACTURING ANTIREFLECTION FILM, ANTIREFLECTION FILM, POLARIZING PLATE, AND IMAGE DISPLAY DEVICE</title><author>OKANO MASARU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2009210876A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2009</creationdate><topic>LAYERED PRODUCTS</topic><topic>LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM</topic><topic>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</topic><topic>OPTICS</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICS</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>OKANO MASARU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>OKANO MASARU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR MANUFACTURING ANTIREFLECTION FILM, ANTIREFLECTION FILM, POLARIZING PLATE, AND IMAGE DISPLAY DEVICE</title><date>2009-09-17</date><risdate>2009</risdate><abstract>PROBLEM TO BE SOLVED: To provide an antireflection film which is excellent in chemical resistance, adhesiveness and scuff resistance after moisture and heat treatment such as in a high temperature and high humidity environment, and is inexpensive since properties of a thin film can be improved by forming an antireflection layer made of one low-refractive index layer. SOLUTION: The method for manufacturing antireflection film includes: a process of providing a hard coat layer directly or via other layer on a film base; and further laminating a low-refractive index layer on the hard coat layer, wherein the hard coat layer contains at least one kind of compound having an HLB value of 3 to 18 and, further, the surface of the hard coat layer is surface-treated and, thereafter, the low-refractive index layer containing at least one kind of hollow silica based particles each of which has an outer shell layer and a porous and hollow interior is laminated on the surface of the hard coat layer. COPYRIGHT: (C)2009,JPO&INPIT</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng |
recordid | cdi_epo_espacenet_JP2009210876A |
source | esp@cenet |
subjects | LAYERED PRODUCTS LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT ORNON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS OPTICS PERFORMING OPERATIONS PHYSICS TRANSPORTING |
title | METHOD FOR MANUFACTURING ANTIREFLECTION FILM, ANTIREFLECTION FILM, POLARIZING PLATE, AND IMAGE DISPLAY DEVICE |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-09T22%3A11%3A49IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=OKANO%20MASARU&rft.date=2009-09-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2009210876A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |