POLYPROPYLENIC RESIN COMPOSITION
PROBLEM TO BE SOLVED: To obtain a polypropylenic resin composition having improved surface appearance, coating appearance qualities, a low coefficient of linear expansion and excellent dimensional stability and a molded article thereof. SOLUTION: The polypropylenic resin composition comprises (A) 40...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To obtain a polypropylenic resin composition having improved surface appearance, coating appearance qualities, a low coefficient of linear expansion and excellent dimensional stability and a molded article thereof. SOLUTION: The polypropylenic resin composition comprises (A) 40-85 wt.% of a polypropylene resin that is polymerized by using a metallocene catalyst and has a melt flow rate (MFR) of 1-100 g/10 minutes and a melt peak temperature of 121-150°C, (B) 14.5-59.5 wt.% of a propylene block copolymer having a melt peak temperature of 155-170°C and (C) 0.5-20 wt.% of carbon fiber. COPYRIGHT: (C)2009,JPO&INPIT |
---|