PROPYLENE HOMOPOLYMER AND METHOD FOR PRODUCING THE SAME

PROBLEM TO BE SOLVED: To provide a propylene homopolymer having high melt tension and melt viscoelasticity, good flowability and excellent in moldability owing to a high swelling ratio in blow molding. SOLUTION: The propylene homopolymer has 6 characteristics: (1) 200,000-1,000,000 weight average mo...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: UCHINO HIDEFUMI, ITO MASAAKI, ISHIMOTO YUYA, AOKI MASARU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator UCHINO HIDEFUMI
ITO MASAAKI
ISHIMOTO YUYA
AOKI MASARU
description PROBLEM TO BE SOLVED: To provide a propylene homopolymer having high melt tension and melt viscoelasticity, good flowability and excellent in moldability owing to a high swelling ratio in blow molding. SOLUTION: The propylene homopolymer has 6 characteristics: (1) 200,000-1,000,000 weight average molecular weight (Mw) by GPC, (2) 3.5-10.5 Q value by GPC, (3) ≥1.2 α/β, wherein α=H50-Tp, β=Tp-L50,Tp denotes the common logarithm of a molecular weight corresponding to a peak position of a molecular weight distribution curve by GPC, L50and H50denote the common logarithm of molecular weights corresponding to 50% height of Tp (L50denotes a molecular weight in the lower side than Tp and H50denotes a molecular weight in the higher side than Tp), (4) ≥90% mm fraction, (5) ≤6.0 wt.% component eluted at ≤90°C by TREF and (6) ≥0.1 number of branched carbon atoms per 1000 whole skeleton forming carbon atoms of the propylene polymer by NMR analysis. COPYRIGHT: (C)2007,JPO&INPIT
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2007154121A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2007154121A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2007154121A3</originalsourceid><addsrcrecordid>eNrjZDAPCPIPiPRx9XNV8PD39Q_w94n0dQ1ScPRzUfB1DfHwd1Fw8w9SACpyCXX29HNXCPFwVQh29HXlYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgbmhqYmhkaGjsZEKQIAnPMopg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PROPYLENE HOMOPOLYMER AND METHOD FOR PRODUCING THE SAME</title><source>esp@cenet</source><creator>UCHINO HIDEFUMI ; ITO MASAAKI ; ISHIMOTO YUYA ; AOKI MASARU</creator><creatorcontrib>UCHINO HIDEFUMI ; ITO MASAAKI ; ISHIMOTO YUYA ; AOKI MASARU</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a propylene homopolymer having high melt tension and melt viscoelasticity, good flowability and excellent in moldability owing to a high swelling ratio in blow molding. SOLUTION: The propylene homopolymer has 6 characteristics: (1) 200,000-1,000,000 weight average molecular weight (Mw) by GPC, (2) 3.5-10.5 Q value by GPC, (3) ≥1.2 α/β, wherein α=H50-Tp, β=Tp-L50,Tp denotes the common logarithm of a molecular weight corresponding to a peak position of a molecular weight distribution curve by GPC, L50and H50denote the common logarithm of molecular weights corresponding to 50% height of Tp (L50denotes a molecular weight in the lower side than Tp and H50denotes a molecular weight in the higher side than Tp), (4) ≥90% mm fraction, (5) ≤6.0 wt.% component eluted at ≤90°C by TREF and (6) ≥0.1 number of branched carbon atoms per 1000 whole skeleton forming carbon atoms of the propylene polymer by NMR analysis. COPYRIGHT: (C)2007,JPO&amp;INPIT</description><language>eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><creationdate>2007</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070621&amp;DB=EPODOC&amp;CC=JP&amp;NR=2007154121A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070621&amp;DB=EPODOC&amp;CC=JP&amp;NR=2007154121A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>UCHINO HIDEFUMI</creatorcontrib><creatorcontrib>ITO MASAAKI</creatorcontrib><creatorcontrib>ISHIMOTO YUYA</creatorcontrib><creatorcontrib>AOKI MASARU</creatorcontrib><title>PROPYLENE HOMOPOLYMER AND METHOD FOR PRODUCING THE SAME</title><description>PROBLEM TO BE SOLVED: To provide a propylene homopolymer having high melt tension and melt viscoelasticity, good flowability and excellent in moldability owing to a high swelling ratio in blow molding. SOLUTION: The propylene homopolymer has 6 characteristics: (1) 200,000-1,000,000 weight average molecular weight (Mw) by GPC, (2) 3.5-10.5 Q value by GPC, (3) ≥1.2 α/β, wherein α=H50-Tp, β=Tp-L50,Tp denotes the common logarithm of a molecular weight corresponding to a peak position of a molecular weight distribution curve by GPC, L50and H50denote the common logarithm of molecular weights corresponding to 50% height of Tp (L50denotes a molecular weight in the lower side than Tp and H50denotes a molecular weight in the higher side than Tp), (4) ≥90% mm fraction, (5) ≤6.0 wt.% component eluted at ≤90°C by TREF and (6) ≥0.1 number of branched carbon atoms per 1000 whole skeleton forming carbon atoms of the propylene polymer by NMR analysis. COPYRIGHT: (C)2007,JPO&amp;INPIT</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2007</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAPCPIPiPRx9XNV8PD39Q_w94n0dQ1ScPRzUfB1DfHwd1Fw8w9SACpyCXX29HNXCPFwVQh29HXlYWBNS8wpTuWF0twMSm6uIc4euqkF-fGpxQWJyal5qSXxXgFGBgbmhqYmhkaGjsZEKQIAnPMopg</recordid><startdate>20070621</startdate><enddate>20070621</enddate><creator>UCHINO HIDEFUMI</creator><creator>ITO MASAAKI</creator><creator>ISHIMOTO YUYA</creator><creator>AOKI MASARU</creator><scope>EVB</scope></search><sort><creationdate>20070621</creationdate><title>PROPYLENE HOMOPOLYMER AND METHOD FOR PRODUCING THE SAME</title><author>UCHINO HIDEFUMI ; ITO MASAAKI ; ISHIMOTO YUYA ; AOKI MASARU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2007154121A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2007</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>UCHINO HIDEFUMI</creatorcontrib><creatorcontrib>ITO MASAAKI</creatorcontrib><creatorcontrib>ISHIMOTO YUYA</creatorcontrib><creatorcontrib>AOKI MASARU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>UCHINO HIDEFUMI</au><au>ITO MASAAKI</au><au>ISHIMOTO YUYA</au><au>AOKI MASARU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PROPYLENE HOMOPOLYMER AND METHOD FOR PRODUCING THE SAME</title><date>2007-06-21</date><risdate>2007</risdate><abstract>PROBLEM TO BE SOLVED: To provide a propylene homopolymer having high melt tension and melt viscoelasticity, good flowability and excellent in moldability owing to a high swelling ratio in blow molding. SOLUTION: The propylene homopolymer has 6 characteristics: (1) 200,000-1,000,000 weight average molecular weight (Mw) by GPC, (2) 3.5-10.5 Q value by GPC, (3) ≥1.2 α/β, wherein α=H50-Tp, β=Tp-L50,Tp denotes the common logarithm of a molecular weight corresponding to a peak position of a molecular weight distribution curve by GPC, L50and H50denote the common logarithm of molecular weights corresponding to 50% height of Tp (L50denotes a molecular weight in the lower side than Tp and H50denotes a molecular weight in the higher side than Tp), (4) ≥90% mm fraction, (5) ≤6.0 wt.% component eluted at ≤90°C by TREF and (6) ≥0.1 number of branched carbon atoms per 1000 whole skeleton forming carbon atoms of the propylene polymer by NMR analysis. COPYRIGHT: (C)2007,JPO&amp;INPIT</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2007154121A
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVINGCARBON-TO-CARBON UNSATURATED BONDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
title PROPYLENE HOMOPOLYMER AND METHOD FOR PRODUCING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-08T10%3A59%3A14IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=UCHINO%20HIDEFUMI&rft.date=2007-06-21&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2007154121A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true