DEPOSITION FRICTION STIR WELDING PROCESS AND ASSEMBLY

PROBLEM TO BE SOLVED: To provide a deposition friction stir welding process that compensates for the production of flash and general thinning of material along the joint line as well as a relatively smooth transition from the non-weld regions to the welded region. SOLUTION: This welding process incl...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: MIKA DAVID PETER
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MIKA DAVID PETER
description PROBLEM TO BE SOLVED: To provide a deposition friction stir welding process that compensates for the production of flash and general thinning of material along the joint line as well as a relatively smooth transition from the non-weld regions to the welded region. SOLUTION: This welding process includes placing a filler material (34) on and about a joint line (16) formed by butting a first workpiece surface (18) against a second workpiece surface (20); and frictionally heating the filler material (34) to soften the filler material (34) and portions of the first and second workpiece surfaces (18, 20) in thermal contact with the filler material (34) and form a weld between the first and second workpieces (18, 20), wherein frictionally heating is at a temperature below a melting point of the filler material (34) and the first and second workpiece surfaces (18, 20). COPYRIGHT: (C)2007,JPO&INPIT
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2007144519A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2007144519A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2007144519A3</originalsourceid><addsrcrecordid>eNrjZDB1cQ3wD_YM8fT3U3AL8nQGM4JDPIMUwl19XDz93BUCgvydXYODFRz9XBQcg4NdfZ18InkYWNMSc4pTeaE0N4OSm2uIs4duakF-fGpxQWJyal5qSbxXgJGBgbmhiYmpoaWjMVGKAFZiKEw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>DEPOSITION FRICTION STIR WELDING PROCESS AND ASSEMBLY</title><source>esp@cenet</source><creator>MIKA DAVID PETER</creator><creatorcontrib>MIKA DAVID PETER</creatorcontrib><description>PROBLEM TO BE SOLVED: To provide a deposition friction stir welding process that compensates for the production of flash and general thinning of material along the joint line as well as a relatively smooth transition from the non-weld regions to the welded region. SOLUTION: This welding process includes placing a filler material (34) on and about a joint line (16) formed by butting a first workpiece surface (18) against a second workpiece surface (20); and frictionally heating the filler material (34) to soften the filler material (34) and portions of the first and second workpiece surfaces (18, 20) in thermal contact with the filler material (34) and form a weld between the first and second workpieces (18, 20), wherein frictionally heating is at a temperature below a melting point of the filler material (34) and the first and second workpiece surfaces (18, 20). COPYRIGHT: (C)2007,JPO&amp;INPIT</description><language>eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2007</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070614&amp;DB=EPODOC&amp;CC=JP&amp;NR=2007144519A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070614&amp;DB=EPODOC&amp;CC=JP&amp;NR=2007144519A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MIKA DAVID PETER</creatorcontrib><title>DEPOSITION FRICTION STIR WELDING PROCESS AND ASSEMBLY</title><description>PROBLEM TO BE SOLVED: To provide a deposition friction stir welding process that compensates for the production of flash and general thinning of material along the joint line as well as a relatively smooth transition from the non-weld regions to the welded region. SOLUTION: This welding process includes placing a filler material (34) on and about a joint line (16) formed by butting a first workpiece surface (18) against a second workpiece surface (20); and frictionally heating the filler material (34) to soften the filler material (34) and portions of the first and second workpiece surfaces (18, 20) in thermal contact with the filler material (34) and form a weld between the first and second workpieces (18, 20), wherein frictionally heating is at a temperature below a melting point of the filler material (34) and the first and second workpiece surfaces (18, 20). COPYRIGHT: (C)2007,JPO&amp;INPIT</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2007</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDB1cQ3wD_YM8fT3U3AL8nQGM4JDPIMUwl19XDz93BUCgvydXYODFRz9XBQcg4NdfZ18InkYWNMSc4pTeaE0N4OSm2uIs4duakF-fGpxQWJyal5qSbxXgJGBgbmhiYmpoaWjMVGKAFZiKEw</recordid><startdate>20070614</startdate><enddate>20070614</enddate><creator>MIKA DAVID PETER</creator><scope>EVB</scope></search><sort><creationdate>20070614</creationdate><title>DEPOSITION FRICTION STIR WELDING PROCESS AND ASSEMBLY</title><author>MIKA DAVID PETER</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2007144519A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2007</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>MIKA DAVID PETER</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MIKA DAVID PETER</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>DEPOSITION FRICTION STIR WELDING PROCESS AND ASSEMBLY</title><date>2007-06-14</date><risdate>2007</risdate><abstract>PROBLEM TO BE SOLVED: To provide a deposition friction stir welding process that compensates for the production of flash and general thinning of material along the joint line as well as a relatively smooth transition from the non-weld regions to the welded region. SOLUTION: This welding process includes placing a filler material (34) on and about a joint line (16) formed by butting a first workpiece surface (18) against a second workpiece surface (20); and frictionally heating the filler material (34) to soften the filler material (34) and portions of the first and second workpiece surfaces (18, 20) in thermal contact with the filler material (34) and form a weld between the first and second workpieces (18, 20), wherein frictionally heating is at a temperature below a melting point of the filler material (34) and the first and second workpiece surfaces (18, 20). COPYRIGHT: (C)2007,JPO&amp;INPIT</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JP2007144519A
source esp@cenet
subjects CLADDING OR PLATING BY SOLDERING OR WELDING
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title DEPOSITION FRICTION STIR WELDING PROCESS AND ASSEMBLY
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-22T06%3A57%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MIKA%20DAVID%20PETER&rft.date=2007-06-14&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2007144519A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true